负弯矩区钢梁上部预制混凝土板U形搭接钢筋湿接缝承载性能研究OA
Study on resistance of wet connection with U-shape-lapped rebar between precast concrete slabs on steel beam in hogging moment region
针对钢梁上部负弯矩区预制混凝土楼板U形搭接钢筋湿接缝的受弯性能,选取湿接缝宽度、U形钢筋间距、插筋面积、面层厚度及U形筋搭接长度等参数,设计了 6个钢梁上侧U形搭接钢筋湿接缝节点并进行三点加载试验.试验结果表明:节点主要呈现弯曲破坏与剪切破坏两种破坏模式,U形搭接钢筋湿接缝节点承载力与延性均高于整体现浇节点;减小U形搭接钢筋间距可显著提升节点的承载力与延性;建筑面层可有效抑制节点区域预制板与现浇混凝土间的裂缝发展.通过有限元模拟,进一步分析了混凝土强度等级、钢筋等级、钢筋直径及搭接长度等参数对节点承载力的影响:当搭接长度不足时,压杆混凝土会过早强度破坏,进而降低节点区拉、压杆传力效率;湿接缝混凝土强度和接缝宽度对受弯承载力影响较小;U形钢筋截面面积与强度等级对承载力影响显著,且在特定范围内钢筋截面面积与受弯承载力呈近似线性相关.基于拉压杆模型与正截面受力平衡理论,推导了适用于该节点的承载力计算公式,计算结果与试验值及有限元结果吻合良好,偏差均小于10%.
The flexural performance of wet joints with U-shaped-lapped rebars between precast concrete slabs on steel beams under hogging moments was investigated.Taking the width of the wet joint,the spacing of the U-shaped rebars,the area of the inserted rebars,the thickness of the surface layer,and the lap length of the U-shaped rebars as parameters,six specimens of joints with U-shaped-lapped rebars on steel beams were designed and three-point loading tests were conducted.According to the test results,the joints primarily exhibit two failure modes:flexural failure and shear failure.The bearing capacity and ductility of wet joints with U-shaped-lapped rebars are both higher than those of monolithic cast-in-place joints.Reducing the spacing between U-shaped-lapped rebars can significantly improve the flexural resistance and ductility of joints.The surface layer can effectively suppress the expansion of cracks between precast slabs and cast-in-place concrete in the joint area.Through finite element simulations,the influence of parameters,including concrete strength grade,reinforcement grade,rebar diameter,and lap length,on the resistance of the joints was further analyzed.When the lap length is insufficient,the concrete in the compression strut will fail prematurely,thereby reducing the force-transfer efficiency of the tension ties and compression struts in the joint area.The strength and joint width of wet-joint concrete have a minor impact on the flexural capacity.The cross-sectional area and strength grade of U-shaped rebars significantly affect the bearing capacity,and within a specific range,there is an approximate linear correlation between the cross-sectional area of steel rebars and the flexural bearing capacity.Based on the strut-and-tie model and the equilibrium theory of normal section forces,a moment resistance calculation formula for the proposed joint was derived.The calculation results agreed well with the experimental and finite element results,with deviations less than 10%.
刘学春;张文博;陈学森;周伟;冯徐泽;李照祺;王广为
北京工业大学北京市高层大跨预应力钢结构工程研究中心,北京 100124北京工业大学北京市高层大跨预应力钢结构工程研究中心,北京 100124北京工业大学北京市高层大跨预应力钢结构工程研究中心,北京 100124北京工业大学北京市高层大跨预应力钢结构工程研究中心,北京 100124北京工业大学北京市高层大跨预应力钢结构工程研究中心,北京 100124中铁建设集团有限公司,北京 100040中铁建设集团有限公司,北京 100040
建筑与水利
预制板湿接缝节点U形搭接钢筋负弯矩区有限元模型受弯承载力
precast slabwet jointU-shaped-lapped rebarnegative moment regionfinite element modelflexural capacity
《建筑结构学报》 2026 (9)
82-93,12
北京市自然科学基金项目(8222007).