首页|期刊导航|建筑结构学报|预制钢筋超高性能混凝土模壳混凝土梁柱节点受剪性能研究

预制钢筋超高性能混凝土模壳混凝土梁柱节点受剪性能研究OA

Shear performance of concrete beam-column joints with precast reinforced ultra-high performance concrete shells

中文摘要英文摘要

为研究预制钢筋超高性能混凝土(ultra-high performance concrete,UHPC)模壳混凝土梁柱节点的破坏机理与受力性能,通过拟静力试验对6个边节点试件的受剪性能进行了研究.试验参数包括预制柱模壳厚度、柱轴压比和节点核心区配箍率等,考察了节点的破坏模式和裂缝开展情况,分析了各参数对滞回曲线、承载能力以及耗能能力等的影响.研究结果表明:试件的最终破坏以节点核心区剪切破坏为主,同时,梁柱交界面以及节点核心区模壳与核心混凝土界面均出现不同程度的分离;柱模壳厚度的增加使得节点核心区开口处的模壳对核心混凝土的有效约束范围减少,从而加速了界面黏结的退化;当柱模壳厚度从30 mm增加到50 mm时,试件的峰值荷载仅提高了 4.66%;随着柱轴压比的增加,模壳对核心混凝土的约束作用增强,试件的开裂荷载和峰值荷载均有明显提升;当节点核心区配箍率从0.85%增加至1.06%时,试件的峰值荷载提高了 6.62%,提高配箍率能有效延缓界面的黏结退化,高配箍率试件的界面黏结退化最小,对应的界面完整性最好.基于斜压杆-桁架模型提出了节点的受剪承载力计算方法,计算结果与试验结果总体吻合较好.

To investigate the failure mechanisms and mechanical behavior of reinforced concrete beam-column joints with precast ultra-high performance concrete(UHPC)shells,quasi-static tests were conducted on six exterior joints to evaluate their shear behavior.The experimental parameters included the thickness of the precast column UHPC shell,the axial compression ratio of column,and the joint core stirrup ratio.The failure modes and crack propagation of the joints were examined in detail,and the influences of these parameters on the hysteretic curves,load-bearing capacity,and energy dissipation capacity were analyzed.The results indicate that the final failure is primarily characterized by shear failure in the joint core,accompanied by varying degrees of debonding at the beam-column interface and the UHPC shell-core concrete interface.The increase in UHPC shell thickness reduces the effective confinement range of the UHPC shell on the core concrete at the joint opening,thereby accelerating the degradation of interfacial bond strength.As the shell thickness increases from 30 mm to 50 mm,the peak load increases by only 4.66%.With the increase of axial compression ratio,the confinement effect of the UHPC shell on the core concrete is enhanced,and both the cracking load and peak load of the specimen increase significantly.The peak load of the specimen increases by 6.62%when the stirrup ratio increases from 0.85%to 1.06%.Furthermore,increasing the stirrup ratio effectively slows down the degradation rate of interfacial bond strength.The specimen with a higher stirrup ratio exhibits the smallest interfacial bond degradation,indicating the best interfacial integrity.Finally,a shear capacity calculation method was proposed based on the strut-and-truss model,showing good agreement between calculated and experimental results.

王朋;尤学辉;史庆轩;王秋维;戎翀

西安建筑科技大学土木工程学院,陕西西安 710055||西安建筑科技大学结构工程与抗震教育部重点实验室,陕西西安 710055西安建筑科技大学土木工程学院,陕西西安 710055西安建筑科技大学土木工程学院,陕西西安 710055||西安建筑科技大学结构工程与抗震教育部重点实验室,陕西西安 710055西安建筑科技大学土木工程学院,陕西西安 710055||西安建筑科技大学结构工程与抗震教育部重点实验室,陕西西安 710055西安建筑科技大学土木工程学院,陕西西安 710055||西安建筑科技大学结构工程与抗震教育部重点实验室,陕西西安 710055

建筑与水利

梁柱节点钢筋UHPC模壳拟静力试验受剪性能承载力计算

beam-column jointreinforced UHPC shellquasi-static testshear performancecalculation of bearing capacity

《建筑结构学报》 2026 (9)

14-28,15

国家自然科学基金项目(52578245),陕西省自然科学基础研究实验室重点项目(2025SYS-SYSZD-048).

10.14006/j.jzjgxb.2026.0135

评论