中文摘要英文摘要

为研究火灾短时高温对邻近电缆交联聚乙烯(XLPE)绝缘理化性能的影响,该文首先通过仿真分析隧道发生火灾时电缆绝缘层的受热特征,然后搭建具备无氧环境与温控功能的短时高温处理平台,依据仿真结果对 XLPE 试样进行峰值温度为 120~400℃的模拟火灾短时高温处理,从微观、力学、电气等方面分析不同 XLPE 试样的理化性能的变化规律.结果表明,火灾过程作用时间短,与常规热老化 XLPE 在长期高温作用下发生热氧降解导致的性能变化不同.当处理温度为 120℃和 160℃时,XLPE 发生重结晶现象,部分理化性能有所改善;200℃处理后 XLPE的热降解现象加剧,整体性能开始下降,但下降幅度小,劣化程度较轻;300℃处理后 XLPE 的力学性能与介电常数出现突变现象,此时劣化程度加剧;当温度升高至 350℃和 400℃时,XLPE 球晶结构出现明显缺陷,且力学性能与击穿场强的下降幅度显著增大,XLPE 发生严重劣化.

Prolonged operation leads to performance degradation of power cables,increasing the risk of joint breakdown and fire.While fire protection measures in tunnels effectively shield adjacent cables from direct flame impingement,these cables may still suffer insulation degradation or even failure due to exposure to high-temperature environments during a fire.Currently,research on the temperature evolution of the insulation layer during cable tunnel fires is limited,leaving the resulting changes in cable insulation performance poorly understood.This study investigates the changes in the physical and chemical properties of cross-linked polyethylene(XLPE),under simulated fire conditions,analyzing its performance after exposure to different short-term high temperatures. First,a simulation model of a cable tunnel was established based on typical structural features to analyze the temperature evolution of the insulation layer from fire detection to extinguishment.Considering the non-uniform temperature distribution across the insulation layer,the cases where the peak insulation layer temperature reached approximately 120,160,200,250,300,350,and 400℃,respectively,were selected as the basis for subsequent short-term high-temperature treatments on XLPE.Then,an oxygen-free,temperature-controlled platform was constructed to subject XLPE samples to short-term high-temperature treatments following the simulated temperature-time curves,replicating the thermal exposure of cable insulation during a fire.Finally,the physical and chemical properties of the treated XLPE samples were analyzed using Fourier transform infrared spectroscopy(FTIR),scanning electron microscopy(SEM),X-ray diffraction(XRD),differential scanning calorimetry(DSC),gel content measurement,tensile testing,frequency-domain dielectric spectroscopy,DC conductivity measurement,and breakdown strength testing. The results indicate that the short-term high temperature exposure during a fire differs from the performance changes caused by long-term thermal-oxidative degradation in conventional thermal aging.After treatment at 120℃and 160℃,XLPE underwent recrystallization,leading to improvement in certain physical and chemical properties.The thermal degradation phenomenon intensified after treatment at 200℃,and the overall performance began to decline,but the degree of degradation was relatively mild.Treatment at 300℃resulted in intensified deterioration,accompanied by a sudden change in mechanical properties and dielectric constant.At 350℃and 400℃,XLPE experienced severe deterioration,exhibiting obvious defects in the spherulite structure and a significant decrease in both mechanical properties and breakdown field strength.

普子恒;李襟愉;王帅;任志刚;郭卫

三峡大学电气与新能源学院 宜昌 443002三峡大学电气与新能源学院 宜昌 443002国网北京市电力公司电力科学研究院 北京 100075国网北京市电力公司电力科学研究院 北京 100075国网北京市电力公司电力科学研究院 北京 100075

信息技术与安全科学

电缆通道火灾模拟极端高温交联聚乙烯理化性能

Cable tunnelfire simulationextreme temperaturescross-linked polyethylenephysical and chemical properties

《电工技术学报》 2026 (20)

6872-6884,13

国家电网有限公司总部管理科技资助项目(520201250016-159-ZN).

10.19595/j.cnki.1000-6753.tces.251919