CO2-盐水-岩石反应对盖层突破压力影响的试验研究OA
Experimental study of the effect of CO2-brine-rock interactions on the breakthrough pressure of caprock
突破压力是表征盖层毛细密封能力的关键参数.CO2注入引发的CO2-盐水-岩石反应会显著影响岩石的输运和密封特性,但该作用对盖层突破压力的影响机制尚不清楚.为揭示盖层突破压力对CO2-盐水-岩石反应的响应机制,利用取自于准噶尔盆地的深部盖层岩心,开展CO2-盐水-岩石反应过程中盖层突破压力测试,并采用核磁共振、显微电子扫描、液相离子色谱及静态水滴法等手段,表征岩心的孔隙结构及润湿性演化特征.结果表明,CO2-盐水-岩石反应导致盖层突破压力降低,这一现象可归因于岩心孔隙体积增加、渗透性增强及润湿性减弱的协同驱动作用.通过矿物溶蚀反应动力学分析发现,在次生矿物阻抗效应作用下,随着反应时长的增加,盖层突破压力降幅将逐步减缓并趋于稳定.在地质封存工程安全运行压力阈值设计中,需充分考量CO2-盐水-岩石反应引发的盖层密封性能减弱效应,以保障工程的长期安全与稳定运行.
Breakthrough pressure serves as a critical parameter for characterizing the capillary sealing capacity of caprock formations.The injection of CO2 into subsurface reservoirs triggers complex interactions among CO2,formation brine and rock.These interactions have been shown to significantly affect the rock's transport properties and sealing performance.However,the mechanisms by which CO2-brine-caprock interactions affect caprock breakthrough pressure remain poorly understood.To elucidate the response mechanism of caprock breakthrough pressure to CO2-brine-rock interactions,breakthrough pressure experiments were performed over different durations of CO2-brine-rock interaction,utilizing two distinct types of caprock cores obtained from the Junggar Basin.A suite of complementary analytical methods,including nuclear magnetic resonance,scanning electron microscopy,liquid chromatography,and contact angle measurements,was employed to characterize the evolution of pore structure and wettability within the cores.The results show that CO2-brine-rock interactions reduce the breakthrough pressure of the caprock samples.This reduction is attributed to the combined effects of increased pore volume,enhanced permeability,and diminished wettability.Further kinetic analysis of mineral dissolution suggests that the decline in breakthrough pressure slows over time and may eventually reach a steady state.This behavior is likely attributable to the inhibitory effect of secondary mineral precipitation.These finding underscore the critical importance of accounting for CO2-brine-rock-induced degradation of caprock sealing capacity when defining pressure thresholds for the safe operation of CO2 geological storage projects,thereby helping to ensure long-term stability and safety.
王兴华;程鹏举;侯赟璐;靳军;高文彬;谭永胜;张琦;李琦
中国石油新疆油田公司,新疆克拉玛依 834000||新疆维吾尔自治区油气田环保节能工程研究中心,新疆克拉玛依 834000中国科学院武汉岩土力学研究所岩土力学与工程安全全国重点实验室,湖北武汉 430071中国科学院武汉岩土力学研究所岩土力学与工程安全全国重点实验室,湖北武汉 430071中国石油新疆油田公司,新疆克拉玛依 834000||新疆维吾尔自治区油气田环保节能工程研究中心,新疆克拉玛依 834000中国科学院武汉岩土力学研究所岩土力学与工程安全全国重点实验室,湖北武汉 430071中国科学院武汉岩土力学研究所岩土力学与工程安全全国重点实验室,湖北武汉 430071中国石油新疆油田公司,新疆克拉玛依 834000||新疆维吾尔自治区油气田环保节能工程研究中心,新疆克拉玛依 834000中国科学院武汉岩土力学研究所岩土力学与工程安全全国重点实验室,湖北武汉 430071
建筑与水利
CO2地质封存盖层突破压力CO2-盐水-岩石反应
CO2 geological storagecaprockbreakthrough pressureCO2-brine-rock interactions
《岩土力学》 2026 (9)
3041-3051,11
湖北省自然科学基金(No.JCZRQN202500299)中国博士后基金(No.2025M770440)国家自然科学基金(No.42502253,No.12302344).This work was supported by the Natural Science Foundation of Hubei Province(JCZRQN202500299),China Postdoctoral Science Foundation(2025M770440)and the National Natural Science Foundation of China(42502253,12302344).