不同热处理工艺下大直径NiTi-SMA棒材的超弹性试验研究OA
Experimental analysis on superelasticity of large-diameter NiTi-SMA bars under different heat treatment processes
在阻尼元件中添加大直径超弹性NiTi形状记忆合金(NiTi-SMA)棒能使其获得良好的自复位能力,但SMA材料对温度具有较高敏感性,不同的热处理工艺对NiTi-SMA棒的力学性能影响较大,导致含NiTi-SMA棒材阻尼器或支撑的耗能能力及自复位能力受到不同程度的影响,故有必要探究不同热处理工艺对大直径NiTi-SMA棒材力学性能的影响.首先对7根工作段直径均为9 mm的NiTi形状记忆合金棒(镍含量为59.9%)进行不同工艺热处理,然后进行增幅循环拉伸试验,研究不同热处理工艺和增幅循环拉伸对试件的应力-应变关系、残余应变、耗能能力等性能的影响.结果表明:适当热处理能显著提高NiTi-SMA棒材的超弹性,其应力-应变曲线呈典型的旗帜形,工作直径为9 mm的NiTi-SMA棒材的最佳热处理温度和时长分别为400℃和30 min,且越接近该热处理工艺,试件的耗能能力、割线刚度及等效阻尼比越稳定.
The addition of large-diameter hyperelastic NiTi shape memory alloy(NiTi-SMA)bars to damping elements has been demonstrated to achive effective self-centring capability.However,given the high sensitivity of SMA materials to temperature,it is important to note that different heat treatment processes can have a certain impact on the mechanical properties of NiTi-SMA bars.This,in turn,can result in varying degrees of influence on the energy dissipation and self-centering ability of dampers or supports containing NiTi-SMA bars.It is therefore essential to conduct a thorough investigation into the impact of diverse heat treatment processes on the mechanical properties of large-diameter NiTi-SMA bars.This article first conducted different heat treatment processes on seven Ni-59.9%at Ti bars with a working section diameter of nine mm,followed by amplified cyclic tensile tests to investigate the effects of different heat treatment processes on the stress-strain relationship,residual strain,energy dissipation capacity,and other properties of the specimens.The research results indicate that appropriate heat treatment can significantly improve the superelasticity of NiTi-SMA bars,with typical flag-shaped stress-strain curves.The present study investigates the effects of heat treatment temperature and duration on the properties of NiTi-SMA bars with a working diameter of nine mm.The results demonstrate that the optimal heat treatment process for these bars is 400℃for 30 minutes.It is observed that as the heat treatment process approaches the optimal value,the energy dissipation capacity,secant stiffness,and equivalent damping ratio of the specimens exhibit increased stability.
田鹏刚;温景北;杨汶杰;刘康宁;王佳佳;熊二刚
陕西建工控股集团未来城市创新科技有限公司,西安 712000||未来城市建设与管理创新联合研究中心,西安 712000长安大学 建筑工程学院,西安 710061陕西建工控股集团未来城市创新科技有限公司,西安 712000||未来城市建设与管理创新联合研究中心,西安 712000陕西建工控股集团未来城市创新科技有限公司,西安 712000||未来城市建设与管理创新联合研究中心,西安 712000陕西建工控股集团未来城市创新科技有限公司,西安 712000||未来城市建设与管理创新联合研究中心,西安 712000长安大学 建筑工程学院,西安 710061
建筑与水利
形状记忆合金增幅循环拉伸试验热处理超弹性自复位
shape memory alloyamplified cyclic tensile testheat treatmenthyperelasticityself-centering