首页|期刊导航|沈阳工业大学学报|附加纯镍过渡层CMT焊接铝/钛异种金属

附加纯镍过渡层CMT焊接铝/钛异种金属OA

Cold metal transfer welding of aluminum/titanium dissimilar metals with additional pure nickel transition layer

中文摘要英文摘要

[目的]铝/钛异种金属焊接接头能将铝合金与钛合金的优点进行结合,不仅具备低密度、高比强度、耐腐蚀等特性,还具有出色的导电和传热能力,因此在航空、航天、汽车、电子和轮船等多个领域得到了广泛应用.铝/钛异种材料构件的制造在技术上的难点为铝合金与钛合金之间显著的物理化学性质差异和冶金不相容性.直接焊接会在焊缝中产生大量的TiAl3、TiAl2、TiAl等脆硬的金属间化合物,易在熔池凝固过程中引发焊接热裂纹.为提升铝/钛异种金属焊接接头性能,本文在焊缝中引入纯镍过渡层,调控焊缝冶金反应,同时降低低熔点母材侧焊接热输入.[方法]选用4 mm厚5052铝合金与Ti6Al4V钛合金作为母材,在铝合金焊接端面贴敷0.1 mm厚纯镍条作为过渡层,采用直径1.2 mm的Ti6Al4V焊丝作为填充材料,选用CMT焊接方法;经多次参数优化,确定最优焊接参数为送丝速度6 m/min,焊接速度15 cm/min,分别开展使用、不使用纯镍过渡层的对照试验,焊后对接头微观组织及力学性能开展分析.[结果]结果表明,未采用过渡层时焊后无法获得完整有效接头,焊缝中存在未熔合、未焊透等焊接缺陷;凝固阶段高熔点母材生成的树枝晶向低熔点母材内部延伸,形成渗透裂纹.采用纯镍过渡层时,铝/钛异种金属焊后可获得成型完好的焊接接头,宏观检测与微观分析均未检出焊接缺陷;过渡层在焊接过程中完全熔化,焊后原位形成厚度约300 μm元素混合区,借助XRD、SEM、TEM等现代分析检测手段,证实该区域发生三元系反应,主要相产物为AlNi2Ti、NiTi2、Al3Ni2、Al3Ni;接头拉伸试样均断裂于焊缝区,平均抗拉强度为62 MPa.[结论]采用CMT焊接技术焊接铝/钛异种金属,在铝合金母材焊接端面贴敷0.1 mm厚纯镍带作为过渡层,所得接头无焊接缺陷;过渡层在焊接过程中完全熔化并参与焊缝冶金反应,原位生成厚度约300 μm的元素混合区,焊缝中主要的冶金反应及物相在此区域生成.过渡层的引入可有效降低低熔点母材侧热输入,避免焊缝生成大量Ti-Al系脆性金属间化合物而诱发焊接缺陷;相较于未添加纯镍过渡层的焊接接头,采用过渡层后熔池流动性有所提升,焊接板材背面实现焊透.

[Objective]Welded joints of aluminum/titanium dissimilar metals can combine the advantages of aluminum alloys and titanium alloys,having low density,high specific strength,corrosion resistance,and other characteristics,and exhibiting excellent electrical conductivity and heat transfer capabilities.Thus,they have been widely used in aerospace,automotive,electronics,ships,and other fields.The technical difficulties in the manufacture of aluminum/titanium dissimilar material components lie in the significant differences in physical and chemical properties and metallurgical incompatibility between aluminum alloys and titanium alloys.Direct welding will produce a large number of brittle and hard intermetallic compounds such as TiAl3,TiAl2,and TiAl in the weld,resulting in welding hot cracking during the solidification process of the molten pool.To improve the performance of the welded joints of aluminum/titanium dissimilar metals,a pure nickel transition layer was adopted to the weld,which regulated the metallurgical reaction in the weld and reduced the welding heat input on the low-melting-point base material side.[Methods]The base materials were 4 mm thick 5052 aluminum alloy and Ti6Al4V titanium alloy.A 0.1 mm thick pure nickel strip,as a transition layer,was applied to the welding end surface of the aluminum alloy,and Ti6Al4V welding wire with a diameter of 1.2 mm was used as the filling material.The cold metal transfer(CMT)welding method was adopted.After multiple rounds of parameter optimization,the optimal welding parameters were determined to be the wire feed rate of 6 m/min and the welding speed of 15 cm/min.Comparative tests were carried out with and without a pure nickel transition layer,and the microstructure and mechanical properties of the joints were analyzed after welding.[Results]The results show that complete and effective joints cannot be obtained after welding without the use of the transition layer,and there are welding defects such as non-fusion and non-penetration in the weld.Dendrites formed from the high-melting-point base material extend into the low-melting-point base material in the solidification process,which results in the formation of penetrating cracks.Complete and good welded joints are obtained after welding of aluminum/titanium dissimilar metals with the use of the pure nickel transition layer.No welding defects are found in macroscopic testing and microscopic analysis,and the transition layer is completely melted during the welding process.After welding,the transition layer forms an element mixing zone of about 300 μm in situ.By using X-ray diffraction(XRD),scanning electron microscopy(SEM),transmission electron microscopy(TEM),and other modern analysis and detection methods,it is determined that a ternary reaction occurs in the region,producing AlNi2Ti,NiTi2,Al3Ni2,and Al3Ni as the main phase products.The joints are all broken in the weld zone during the tensile process,with an average tensile strength of 62 MPa.[Conclusions]Aluminum/titanium dissimilar metals were welded using the CMT welding technology.The welding end surface of the aluminum alloy base material was coated with a 0.1 mm thick pure nickel strip as a transition layer.No welding defects exist in the welded joint.The transition layer completely melts during the welding process and participates in the metallurgical reaction in the weld,forming an approximately 300 μm thick element mixing zone in situ,where the major metallurgical reactions occur and the primary phases are formed.The addition of the transition layer can effectively reduce the heat input on the low-melting-point base material side,and avoid the generation of a large number of Ti-Al brittle intermetallic compounds in the weld,which can result in welding defects.Compared with the welded joint without the addition of the pure nickel transition layer,the use of the transition layer improves the fluidity of the molten pool,and achieves welding penetration on the back of the welded plate.

刘政军;宋春辉;刘治宇

沈阳工业大学材料科学与工程学院,辽宁沈阳 110870沈阳工业大学材料科学与工程学院,辽宁沈阳 110870沈阳市市场监管事务服务中心,辽宁沈阳 110179

矿业与冶金

铝/钛焊接焊接过渡层异种金属焊接CMT焊接镍过渡层熔池反应断口形貌金属间化合物

aluminum/titanium weldingwelding transition layerdissimilar metal weldingCMT weldingnickel transition layermolten pool reactionfracture morphologyintermetallic compound

《沈阳工业大学学报》 2026 (5)

73-80,8

辽宁省自然科学基金项目(2024-BS-096).

10.7688/j.issn.1000-1646.2026.05.10

评论