首页|期刊导航|金属加工(热加工)|磁场-冷却复合调控明弧堆焊高铬铸铁熔覆层组织与耐磨性能研究

磁场-冷却复合调控明弧堆焊高铬铸铁熔覆层组织与耐磨性能研究OA

Microstructure and wear resistance of open-arc hardfaced high-chromium cast iron coatings under combined magnetic and cooling fields

中文摘要英文摘要

为提升高铬铸铁明弧堆焊熔覆层在冲击磨损工况下的综合性能,采用稳恒磁场与脉冲磁场分别耦合空冷与水冷工艺制备熔覆层,系统研究了磁场-冷却复合作用对其微观组织、力学性能及耐磨性能的影响.利用扫描电子显微镜(SEM)、X射线衍射仪(XRD)、维氏硬度计及摩擦磨损试验机等设备,对熔覆层的显微组织、物相组成、硬度分布及耐磨性能进行系统表征.结果表明:稳恒磁场通过电磁搅拌作用有效细化晶粒、改善成分偏析,使空冷与水冷熔覆层硬度分别提升至705.1HV与708.5HV.但水冷与强磁场耦合会诱发Cr向热影响区迁移,形成粗大针状马氏体,导致熔合区界面结合强度下降.脉冲磁场虽对硬度提升有限,但有效缓解了Cr迁移问题.磨损试验表明:空冷稳恒磁场试样在滑动磨损中磨痕深度最小,为4.45μm,较无磁场试样降低21.24%;而空冷脉冲磁场试样在冲击磨损中表现出最优抗冲击性能,磨损失重仅为21mg.本研究为破碎机锤头等抗冲击耐磨件的明弧堆焊工艺优化提供了理论依据和技术参考.

To enhance the comprehensive performance of high-chromium cast iron coatings deposited by open-arc hardfacing impact-wear conditions,coatings were prepared under static magnetic field and pulsed magnetic field,under both air-cooled and water-cooled conditions.The synergistic effects of magnetic field and cooling method on microstructure,mechanical properties,and wear resistance were systematically investigated.The microstructure,phase composition,hardness distribution,and wear resistance of the coatings were characterized by scanning electron microscopy(SEM),X-ray diffraction(XRD),Vickers hardness testing,and friction-and-wear testing.The results demonstrate that the static magnetic field effectively refines grains and reduces compositional segregation through electromagnetic stirring,increasing the hardness of air-cooled and water-cooled coatings to 705.1HV and 708.5HV,respectively.However,the coupling of water cooling with an intense static magnetic field promotes chromium migration toward the heat-affected zone,resulting in martensite with coarse acicular morphology and consequently reduced interfacial bonding strength of the fusion zone.Although the pulsed magnetic field does not significantly improve hardness,it effectively mitigates chromium migration.Wear tests indicate that the air-cooled specimen deposited under static magnetic field exhibits the minimum wear depth of 4.45μm under sliding wear,a 21.24%reduction from that of the air-cooled specimen without magnetic field.In contrast,the air-cooled specimen deposited under pulsed magnetic field demonstrates the optimal impact-wear resistance,with a weight loss of 21mg.This study provides a theoretical basis and technical reference for optimizing the open-arc hardfacing process of impact-wear-resistant components such as crusher hammers.

李冰玉;姚鑫;殷子强;温道胜;夏佃秀;陈培敦;彭路

山东电力工程咨询院有限公司 山东济南 250013济南大学机械工程学院 山东济南 250022||山东省金属关键构件表面处理与智能装备重点实验室 山东济南 250022济南大学机械工程学院 山东济南 250022||山东省金属关键构件表面处理与智能装备重点实验室 山东济南 250022济南大学机械工程学院 山东济南 250022||山东省金属关键构件表面处理与智能装备重点实验室 山东济南 250022济南大学机械工程学院 山东济南 250022||山东省金属关键构件表面处理与智能装备重点实验室 山东济南 250022济南大学机械工程学院 山东济南 250022||山东省金属关键构件表面处理与智能装备重点实验室 山东济南 250022山东泓路机械设备制造有限公司 山东济南 250022

明弧堆焊高铬铸铁冷却条件外加磁场耐磨性

open-arc hardfacinghigh-chromium cast ironcooling conditionsexternal magnetic fieldwear resistance

《金属加工(热加工)》 2026 (10)

91-105,112,16

国家自然科学基金资助项目(51305245)山东省自然科学基金资助项目(ZR2020ME150)山东省科技型中小企业创新能力提升工程项目(2024TSG0130、2024TSG0111)济南市"新高校20条"项目(202534079)山东省重点研发计划项目(2026CXPT165).