首页|期刊导航|新疆大学学报(自然科学版中英文)|预制混凝土夹芯保温墙复合型连接件抗剪性能试验

预制混凝土夹芯保温墙复合型连接件抗剪性能试验OA

Experimental Study on Shear Performance of Composite Connectors for Precast Concrete Sandwich Insulation Walls

中文摘要英文摘要

为满足预制混凝土夹芯保温墙体的传力与保温需求,解决传统连接件难以兼顾力学性能与热工性能的问题,设计"钢管-环氧树脂-橡胶-十字钢筋"复合型保温连接件,以保温层厚度(75 mm、95 mm、115 mm)和连接件平面布置形式(1×1、2×1、3×1、2×2)为双控制变量,开展单侧剪切试验,系统探究上述变量对连接件抗剪性能的影响规律.结果表明,在2×2连接件布置形式下,随着保温层厚度从75 mm增至115 mm,单个连接件抗剪承载力从28.66 kN降至20.02 kN,最大降幅达30.1%,核心原因是悬臂段延长使锚固端弯剪应力显著增加;随连接件布置形式从1×1到2×2,界面整体刚度与极限承载力呈线性增长,75 mm保温层条件下,2×2较1×1刚度提升212%,但受锚固不均匀性影响,单个连接件平均承载力最大衰减38.2%,呈数量与效率的非线性关系;保温层通过界面黏结效应发挥应力缓冲作用,S-95-3组对比试验表明,预先去除保温层会使试件抗剪承载力降低17.3%;连接件破坏过程呈"微裂-扩展-峰值-失效"四阶段特征,核心失效模式为钢管弯剪破坏、十字钢筋拔出与混凝土锚固失效的复合模式.保温层厚度与连接件布置形式对复合型连接件抗剪性能影响显著,需平衡连接件数量与效率,以保证保温层界面黏结质量.

To address the issue that traditional connectors struggle to balance mechanical and thermal insulation perfor‐mance,while meeting the force transfer and thermal insulation requirements of precast concrete sandwich insulation walls,a composite thermal insulation connector composed of"steel tube-epoxy resin-rubber-cross steel bar"is designed.Taking the insulation layer thickness(75 mm,95 mm,115 mm)and the planar arrangement of connectors(1×1,2×1,3×1,2×2)as two control variables,unilateral shear tests are conducted to systematically investigate the influence laws of the above variables on the shear performance of the connectors.The test results show that as the insulation layer thickness increases from 75 mm to 115 mm under 2×2 arrangement,the shear bearing capacity of a single connector decreases from 28.66 kN to 20.02 kN,with a maximum reduction of 30.1%.The core reason is that the extension of the cantilever segment significantly increases the bending-shear stress at the anchorage end.As the connector arrangement changes from 1×1 to 2×2,the overall interface stiff‐ness and ultimate bearing capacity show a linear increase.Under the 75 mm insulation layer thickness,compared with the 1×1 arrangement,the stiffness of the 2×2 arrangement increases by 212%.However,affected by uneven anchorage,the average bearing capacity of a single connector decreases by a maximum of 38.2%,presenting a nonlinear relationship between"quan‐tity and efficiency".The insulation layer exerts a stress buffering effect through the interface bonding effect.The comparative test of group S-95-3 shows that pre-removal of the insulation layer reduces the shear bearing capacity of the specimen by 17.3%.The failure process of the connector exhibits four-stage characteristics of"microcracking-propagation-peak-failure",and the core failure mode is a composite mode of steel tube bending-shear failure,cross steel bar pull-out,and concrete an‐chorage failure.The thickness of the insulation layer and the arrangement of connectors have significant influences on the shear performance of the composite connectors.It is necessary to balance the number and efficiency of connectors to ensure the interface bonding quality of the insulation layer.

他维元;姜洪斌;马财龙;周海威;翟新铭

新疆大学 建筑工程学院,新疆 乌鲁木齐 830017哈尔滨工业大学 土木工程学院,黑龙江 哈尔滨 150090新疆大学 建筑工程学院,新疆 乌鲁木齐 830017新疆新冶建筑集成科技有限公司,新疆 乌鲁木齐 830023新疆冶金建设(集团)有限责任公司,新疆 乌鲁木齐 830009

建筑与水利

夹芯保温墙体复合型保温连接件单侧剪切试验布置形式保温层厚度

sandwich insulation wallcomposite insulation connectorunilateral shear testarrangement forminsulation layer thickness

《新疆大学学报(自然科学版中英文)》 2026 (5)

613-624,12

新疆维吾尔自治区区域协同创新专项"新疆装配式混凝土一体化剪力墙关键技术应用研究与工程示范"(2022E02095).