煅烧温度对Ni-ZrO2催化剂甲烷干重整反应催化性能的影响OA
Effects of calcination temperatures on catalytic performances of Ni-ZrO2 catalysts for methane dry reforming
甲烷干重整(DRM)可将CH4和CO2转化为合成气,实现温室气体资源化利用并缓解能源危机.Ni-ZrO2催化剂因活性高、成本低被大量应用于催化DRM反应.其中,煅烧温度作为催化剂制备关键参数,直接影响其结构与催化性能.首先采用共沉淀法制备了不同煅烧温度(700 °C、800 °C和900 °C)的Ni-ZrO2催化剂,采用XRD、TEM和H2-TPR等方法对催化剂进行了表征,筛选了最优煅烧温度,明确了煅烧温度对Ni-ZrO2催化剂结构及DRM反应催化性能的影响.结果表明,800℃下煅烧可以构建适中的Ni-ZrO2相互作用,更重要的是该温度下煅烧可以构造m-ZrO2/c-ZrO2混相异质界面以均匀锚定Ni纳米颗粒.在800 °C、常压和空速36000 mL/(g·h)条件下反应25 h,Ni-ZrO2-800作用下CO2和CH4转化率分别达到88%和81%,且该催化剂保持较高活性和稳定性.相比之下,Ni-ZrO2-700和Ni-ZrO2-900则表现出较低的活性和稳定性,这是由于锚定Ni物种的异质界面位点不足,以及Ni物种被过度包覆.因此,在800 °C的最优煅烧温度下,通过构建混相异质界面及适中金属-载体相互作用,可提升催化剂催化活性与稳定性.本研究可为后续Ni-ZrO2催化剂制备工艺优化及工业化应用提供理论支撑.
Methane dry reforming(DRM)can convert CH4 and CO2 into syngas,realizing the resource utilization of greenhouse gases and alleviating the energy crisis.Ni-ZrO2 catalysts have been extensively used in DRM reaction owing to their high activity and low cost.Calcination temperatures,as a key preparation parameter,directly affect the structures and catalytic performances of catalysts.Ni-ZrO2 catalysts with different calcination temperatures(700℃,800℃and 900℃)were prepared by coprecipitation method,and characterized by methods such as XRD,TEM,and H2-TPR.The optimal calcination temperature was selected and the effects of calcination temperatures on the structures of Ni-ZrO2 catalysts and their catalytic performances for DRM reaction were clarified.The results show that under the calcination temperature of 800℃,moderate Ni-ZrO2 interactions are constructed,and more importantly,m-ZrO2/c-ZrO2 mixed phase heterointerfaces to uniformly anchor Ni nanoparticles are constructed.Under the conditions of 800℃,atmospheric pressure and a space velocity of 36000 mL/(g·h)for 25 hours,the CO2 and CH4 conversion rates achieve 88%and 81%,respectively,with Ni-ZrO2-800,and this catalyst maintains high activity and stability.In contrast,Ni-ZrO2-700 and Ni-ZrO2-900 exhibit low activity and stability,which is attributed to the insufficient heterointerface sites for anchoring Ni species and the excessive encapsulation of Ni species.Therefore,at the optimal calcination temperature of 800℃,the catalytic activity and stability of catalysts can be improved by constructing a mixed phase heterogeneous interface and moderate metal-support interactions.This study can provide theoretical support for the optimization of the preparation process and industrial application of Ni-ZrO2 catalysts in the future.
王楠;李德正;刘小浩
江南大学 化学与材料工程学院,江苏 无锡 214122江南大学 化学与材料工程学院,江苏 无锡 214122江南大学 化学与材料工程学院,江苏 无锡 214122
化学化工
甲烷干重整煅烧温度ZrO2异质界面碳溢流氧空位
methane dry reformingcalcination temperaturesZrO2 heterointerfacescarbon spilloveroxygen vacancies