首页|期刊导航|焊管|厚板钛合金不同空间位置电子束焊接接头组织性能研究

厚板钛合金不同空间位置电子束焊接接头组织性能研究OA

Study on Microstructure and Properties of Electron Beam Welded Joints of Thick-plate Titanium Alloy at Different Spatial Positions

中文摘要英文摘要

为揭示大厚度TC4钛合金构件在不同空间位置下电子束焊接接头组织性能变化机制,以56 mm厚TC4钛合金弧板为研究对象,采用真空动枪电子束焊接技术,开展0°~75°不同空间位置焊接试验,系统探究不同空间位置对焊缝成形、微观组织及力学性能的影响,并结合有限元热过程模拟分析了接头组织性能变化的内在机理.结果显示,电子束焊接可实现钛合金曲面不同空间位置的良好焊缝成形,焊缝区主要由α'马氏体相和β相构成,随角度增大,焊缝微观组织呈"层片状α'→魏氏组织→层片状α'"的演变趋势,α'马氏体长径比从1.8升至峰值4.0(45°位置),后回落至2.8,力学性能呈V形变化,抗拉强度、伸长率、冲击功分别由初始的888 Mpa、18.1%、43.2 J降至45°位置的865 Mpa、13.8%、35.5 J,随后回升至878 Mpa、15.8%、40.5 J.有限元模拟结果显示,0°位置焊接冷却速率明显高于45°位置.结果表明,焊接空间位置通过改变焊接热累积与局部冷却速率调控α'马氏体长径比,进而影响焊缝力学性能,冷却速率越快,α'马氏体长径比越小、层片状组织越细化,焊缝抗拉强度与冲击韧性越优异.

To reveal the evolution mechanism of microstructure and properties for electron beam welded joints of large-thickness TC4 titanium alloy components at different spatial positions,a 56 mm thick TC4 titanium alloy arc plate was taken as the research object.Welding tests at different spatial positions ranging from 0° to 75° were carried out by vacuum moving-gun electron beam welding technology.The effects of welding angle on weld formation,microstructure and mechanical properties were systematically investigated,and the internal mechanism for the variation of joint microstructure and properties was analyzed combined with finite element thermal-process simulation.The results show that favorable weld formation can be obtained at different spatial positions of titanium alloy curved surfaces by electron beam welding.The weld zone is mainly composed of α' martensite phase and β phase.With the increase of welding angle,the weld microstructure presents an evolution trend of lamellar α' → Widmanstätten structure → lamellar α'.The aspect ratio of α' martensite rises from 1.8 to a peak value of 4.0 at 45° position,and then drops to 2.8.The mechanical properties show V-shaped variation.The tensile strength,elongation and impact energy decrease from the initial values of 888 MPa,18.1%and 43.2 J to 865 MPa,13.8%and 35.5 J at 45° position,and then recover to 878 MPa,15.8%and 40.5 J.Finite element simulation results demonstrate that the cooling rate at 0° position is obviously higher than that at 45° position.It is indicated that the welding spatial position can regulate the aspect ratio of α'martensite by changing welding heat accumulation and local cooling rate,and further affect the mechanical properties of welds.A higher cooling rate leads to a smaller aspect ratio of α' martensite and finer lamellar microstructure,which endows the weld with better tensile strength and impact toughness.

张雨龙;杨子威;张浩;贾晓飞;高奇;廖志谦;雷小伟

洛阳船舶材料研究所,河南 洛阳 471023洛阳船舶材料研究所,河南 洛阳 471023洛阳船舶材料研究所,河南 洛阳 471023洛阳船舶材料研究所,河南 洛阳 471023洛阳船舶材料研究所,河南 洛阳 471023洛阳船舶材料研究所,河南 洛阳 471023||海洋腐蚀与防护全国重点实验室,河南 洛阳 471023洛阳船舶材料研究所,河南 洛阳 471023

矿业与冶金

TC4厚板钛合金电子束焊接焊缝成形组织性能冷却速率

TC4 thick-plate titanium alloyelectron beam weldingweld formationmicrostructure and propertiescooling rate

《焊管》 2026 (9)

37-43,50,8

10.19291/j.cnki.1001-3938.2026.09.005

评论