首页|期刊导航|China Foundry|Improvement of microstructure and mechanical properties of Ti_(42)Al_(6)Nb_(2.6)C alloy through Er doping and in-situ formation of Er_(2)O_(3) particles

Improvement of microstructure and mechanical properties of Ti_(42)Al_(6)Nb_(2.6)C alloy through Er doping and in-situ formation of Er_(2)O_(3) particlesOA

中文摘要

The improvement of the morphology and distribution of ceramic particles is a crucial aspect in enhancing the high-temperature strength and service temperature of TiAl-based composites.In this study,the Er element was successfully used to modify the morphology of the Ti_(2)AlC reinforcing phase and improve room-temperature and high-temperature mechanical properties of the alloy.Results show that as the Er content increases from 0.04at.%to 0.08at.%,in-situ Er_(2)O_(3) particles are distributed at the surface of Ti_(2)AlC reinforcing phase and within the lamellar colony.Both the lamellar colony and Ti_(2)AlC reinforcing phase are significantly refined.The orientation relationship between Er_(2)O_(3) and Ti_(2)AlC is{111}_(Er_(2)O_(3))//{0001}_(Ti_(2)AlC) and{110}_(Er_(2)O_(3))//{1121}_(Ti_(2)AlC).The higher surface energy of Ti_(2)AlC and the favorable orientation relationship allow the Er_(2)O_(3) particles to nucleate on the Ti_(2)AlC reinforcing surface.As a result,the growth of Ti_(2)AlC is restricted by the fine Er_(2)O_(3) particles,preventing its uncontrolled expansion and ultimately leading to the formation of fine,short rod-like structures.The fine Er_(2)O_(3) and Ti_(2)AlC act as nucleation sites forβgrains,which is fundamental for obtaining fine lamellar colony.The Ti_(42)Al_(6)Nb_(2.6)C0.08Er alloy exhibits superior room-temperature compressive properties with a compressive strength of 2,106 MPa and a compressive strain of 26.8%.The high-temperature compressive properties also demonstrate a great balance between strength and plasticity.The improvement in compressive properties is attributed to significant changes in microstructures,including the notable refinement of the lamellar colony,precipitation of Er_(2)O_(3) particles,load transfer effect of the refined Ti_(2)AlC reinforcing phase,and solid solution strengthening of Er solutes.

Hong-ze Fang;Ke-xuan Li;Xiao-kang Yang;Hong-yuan Zhai;Xian-fei Ding;Rui-run Chen

National Key Laboratory for Precision Hot Processing of Metals,Harbin Institute of Technology,Harbin 150001,China Zhengzhou Research Institute,Harbin Institute of Technology,Zhengzhou 450000,ChinaNational Key Laboratory for Precision Hot Processing of Metals,Harbin Institute of Technology,Harbin 150001,ChinaNational Key Laboratory for Precision Hot Processing of Metals,Harbin Institute of Technology,Harbin 150001,ChinaNational Key Laboratory for Precision Hot Processing of Metals,Harbin Institute of Technology,Harbin 150001,ChinaCast Titanium Alloy R&D Center,Beijing Institute of Aeronautical Materials,Beijing 100095,China Baimtec Material Co.,Ltd.,Beijing 100094,ChinaNational Key Laboratory for Precision Hot Processing of Metals,Harbin Institute of Technology,Harbin 150001,China Zhengzhou Research Institute,Harbin Institute of Technology,Zhengzhou 450000,China

矿业与冶金

TiAl alloyTi_(2)AlC reinforcing phaserefinementEr_(2)O_(3)particlemechanical properties

《China Foundry》 2026 (5)

P.691-702,12

financial support by the Major Science and Technology Achievement Transformation Project in Heilongjiang Province(No.ZC2023SH0075)the National Natural Science Foundation of China(Nos.52425401,U2441255,52474377,and 52371015)the Young Elite Scientists Sponsorship Program by CAST(No.2021QNRC001)the Henan Provincial Key Research and Development&Promotion Special Program(No.251111231400).

10.1007/s41230-025-5022-0

评论