G20Mn5QT低合金铸件缺欠的焊补工艺研究OA

Study on the Welding Repair Process for G20Mn5QT Low-alloy Casting Steel

中文摘要英文摘要

针对G20Mn5QT低合金铸钢在轨道交通制动夹钳座等关键部件中出现的铸造缺陷,系统研究其高质量焊补修复工艺,以提升缺陷修复质量与构件服役可靠性.G20Mn5QT作为一种广泛应用于转向架、制动系统等关键承载部件的低合金铸钢,其铸造过程中常因工艺波动产生气孔、夹渣、裂纹等缺陷,严重影响构件使用寿命与行车安全.焊补是修复此类缺陷、降低生产成本、提高材料利用率的关键技术手段,但由于G20Mn5QT碳当量较高(0.48~0.64),组织以马氏体为主,焊接过程中易出现热影响区脆化、冷裂纹及残余应力集中等问题,对焊接工艺提出了严格要求.基于此,采用焊条电弧焊方法,选用低氢高韧性焊材ESAB OK48.04,系统研究预热温度、层间温度、热输入等关键参数对焊接接头组织与性能的影响.通过力学性能测试、硬度分析及金相观察,综合评价焊补接头的综合性能.研究表明,在预热(200±10)℃、层间温度210~300 ℃、热输入1.0~1.8kJ/mm的工艺条件下,焊补接头抗拉强度达571 MPa以上,断后伸长率不低于27%,-40 ℃冲击功最高达130 J,焊缝与热影响区硬度分布合理,组织过渡连续,无裂纹、气孔等缺陷.通过优化的焊补工艺,可实现G20Mn5QT铸钢缺陷的高质量修复,接头强度与母材相当,低温韧性显著提升.

A systematic investigation was conducted on an advanced weld repair methodology aimed at rectifying casting defects in critical components,specifically brake calliper brackets manufactured from G20Mn5QT low-alloy cast steel,which are employed in rail transit systems.The primary goal is to improve the quality of defect remediation and enhance the operational reliability of these components.G20Mn5QT,a low-alloy cast steel widely used in vital load-bearing structures such as bogies and braking mechanisms,is prone to casting imperfections,including porosity,slag inclusions,and cracking,largely attributable to process variability.These defects substantially undermine the service life and safety performance of the components.Welding repair constitutes a pivotal approach to address these flaws,thereby lowering production expenses and optimizing material usage.However,the relatively elevated carbon equivalent of G20Mn5QT(ranging from 0.48~0.64),coupled with its predominantly martensitic microstructure,predisposes the welding process to challenges such as embrittlement within the heat-affected zone,cold cracking,and residual stress accumulation,necessitating stringent control over the welding parameters.On this basis,shielded metal arc welding(SMAW)utilizing the low-hydrogen,high-toughness electrode ESAB OK48.04 was employed to systematically evaluate the effects of critical welding parameters,including preheating temperature,interpass temperature,and heat input,on the microstructural characteristics and mechanical performance of the welded joints.Comprehensive assessments were conducted through mechanical testing,hardness profiling,and metallographic examination.The findings reveal that under optimized conditions,specifically,preheating at(200±10)℃,interpassing temperatures between 210 and 300℃,and heat inputs ranging from 1.0 to 1.8 kJ/mm,the weld repairs achieve tensile strengths exceeding 571 MPa,fracture elongations of no less than 27%,and Charpy impact energies at-40℃ reaching up to 130 J.The hardness distribution across the weld metal and heat-affected zone is uniform,with continuous microstructural transitions and an absence of defects such as cracks or porosity.The optimization of the weld repair process facilitates the high-quality restoration of casting defects in G20Mn5QT cast steel,yielding joint strengths comparable to those of the base material and significantly improving the low-temperature toughness.

马凯;边惠惠;魏晓;高志雄;肖骞;李剑波

包头北方创业有限责任公司,内蒙古包头 014030山东劳动职业技术学院,山东济南 250300包头北方创业有限责任公司,内蒙古包头 014030包头北方创业有限责任公司,内蒙古包头 014030||北京交通大学,北京 100044中国铁路北京局集团有限公司,北京 100089中车大连机车车辆有限公司,辽宁大连 116045

矿业与冶金

低合金铸钢焊补热影响区脆化残余应力控制工艺评定

low-alloy cast steelwelding repairheat-affected zone embrittlementresidual stress controlprocess qualification