Effect of Thermal Exposure on the Microstructure Stability of DD10 Single-crystal Superalloy
在航空发动机等关键部件中,高温合金的性能及稳定性直接影响部件的安全性和效率.通过对完全热处理后的DD10单晶高温合金在700和1 100 ℃下进行长时热暴露实验,系统探究不同时效温度及时效时间下,合金中γ'强化相(尺寸、形态、分布)与拓扑密排相(TCP相)的体积分数、形貌特征及演化规律.结果表明,700 ℃热暴露过程中枝晶干和枝晶间的γ'相均只产生了轻微粗化,并未发现有TCP相的析出.随着热暴露温度的升高至1 100 ℃,合金中γ'相的形态发生了显著变化,1 100 ℃下热暴露200h后,γ'相形貌由规则的立方态变成了不规则形态,形成了筏状组织.随热暴露时间的延长,筏化组织逐渐粗化.此外,随着温度升高,难熔元素的偏聚导致μ相的析出.在700和1 100 ℃热暴露过程中,温度越高γ/γ'两相的晶格常数差值越小,两相错配度的绝对值也随之减小.700 ℃热暴露200 h后的错配度略高于热处理态,此时γ'相的立方度也达到最高.
In critical components such as aircraft engines,the performance and stability of high-temperature alloys directly impact component safety and efficiency.Through long-term thermal exposure experiments conducted at 700 and 1 100℃on fully heat-treated DD10 single-crystal superalloys,this study systematically investigated the volume fraction,morphological characteristics,and evolution mechanisms of the γ'strengthening phase(size,morphology,distribution)and topologically close-packed(TCP)phases under different aging temperatures and durations.The results indicate that during 700℃ thermal exposure,only slight coarsening of the γ'phase occurs along the dendrite trunks and interdendritic regions,with no TCP phase precipitation detected.As the thermal exposure temperature increases to 1 100℃,the morphology of the γ'phase in the alloy significantly changes.After 200 h of thermal exposure at 1 100℃,the γ'phase morphology transforms from a regular cubic configuration to an irregular form,resulting in the formation of a rafted structure.With prolonged thermal exposure time,the rafted structure gradually coarsens.Additionally,with increasing temperature,the segregation of refractory elements induces the precipitation of the p phase.During thermal exposure at 700 and 1 100℃,the difference in the lattice constant between the γ and γ'phases decreases with increasing temperature,and the absolute value of the degree of misfit between the two phases also diminishes accordingly.After 200 h of thermal exposure at 700℃,the degree of misfit is slightly greater than that in the as-heat-treated state,and the cubicity of the γ'phase reaches its maximum at this point.
马秀林;黄太文;许佳圣;刘丽君;曹腊梅;苏海军;刘林
西北工业大学凝固技术全国重点实验室,陕西西安 710072西北工业大学凝固技术全国重点实验室,陕西西安 710072西北工业大学凝固技术全国重点实验室,陕西西安 710072中国航发北京航空材料研究院先进高温结构材料重点实验室,北京 100095中国航发北京航空材料研究院先进高温结构材料重点实验室,北京 100095西北工业大学凝固技术全国重点实验室,陕西西安 710072西北工业大学凝固技术全国重点实验室,陕西西安 710072||苏州高晶新材料科技有限公司,江苏苏州 215000
矿业与冶金
镍基单晶高温合金热暴露γ'相TCP相
nickel-based single-crystal superalloythermal exposureγ'phaseTCP phase
《铸造技术》 2026 (8)
879-887,9
重点新材料研发及应用国家科技重大专项(2025ZD0608601)国家科技重大专项(J2019-Ⅶ-0013-0153,2019-Ⅵ-0020-0135)航空发动机及燃气轮机基础科学中心项目(P2021-A-Ⅳ-001-001)陕西省科技计划项目(2021TD-17)