熔体冷速对高铁含量A356铝合金中富铁相尺寸及类型的影响OA
Effect of the Molten Metal Cooling Rate on the Size and Type of Iron-rich Phases in High Iron Containing A356 Al Alloys
原铝生产面临严峻的环境与能源压力,回收利用A356铝合金废料兼具显著的环保和经济价值.然而,废铝再生过程铁元素易过量积累,较低熔体冷速下会形成粗大脆性富铁相,恶化合金力学性能.本研究通过提高熔体冷速优化富铁相的形貌与组成,以铁含量为0.36%(质量分数)的A356铝合金为研究对象,采用不同尺寸的铜模调控熔体冷速(15~108 K/s),对比研究各熔体冷速下富铁相的形貌、尺寸及分布规律.结果表明,随着熔体冷速的提高,富铁相显著细化,分布更趋均匀.相组成分析进一步表明,提高熔体冷速(72~108 K/s)有效抑制了粗大有害相β-Fe的析出,转而促进形成更为细小、对基体割裂作用较弱的π-Fe相.
The primary Al production industry poses significant environmental and energy challenges,making the recycling of A356 Al alloy scrap highly attractive from both ecological and economic perspectives.A critical issue in recycling is the inevitable accumulation of Fe,which leads to the formation of coarse,brittle iron-rich intermetallics at lower solidification cooling rates,severely degrading the mechanical properties.On this basis,the role of increased cooling rates in modifying the morphology and composition of these iron-rich phases was investigated.Using a copper mold technique to achieve a range of cooling rates(15~108 K/s),their impact on the microstructure of an A356 Al alloy containing 0.36 wt.%Fe was systematically examined.The results demonstrate that higher cooling rates significantly refine the iron-rich phases and promote a more uniform distribution.Phase analysis further revealed that at elevated cooling rates(72~108 K/s),the precipitation of the detrimental[3-Fe phase is suppressed,favouring the formation of the less harmful π-Fe phase.
牛云霞;张丽芝;万杰;刘海峰;陈豫增
西北工业大学凝固技术全国重点实验室,陕西西安 710072西北工业大学凝固技术全国重点实验室,陕西西安 710072西北工业大学凝固技术全国重点实验室,陕西西安 710072中信戴卡股份有限公司,河北秦皇岛 066011西北工业大学凝固技术全国重点实验室,陕西西安 710072||西北工业大学宁波研究院,浙江宁波 315103||苏州匀晶金属科技有限公司,江苏苏州 215024
矿业与冶金
高铁含量A356铝合金富铁相熔体冷速微观组织
high-Fe-containing A356 Al alloyiron-rich phasescooling ratemicrostructure
《铸造技术》 2026 (8)
870-878,9
国家重点研发计划(2022YFB3707103)国家自然科学基金(52301197,52071262)凝固技术全国重点实验室自主研究课题(2024-ZD-06,2024-TS-06)中央高校基本科研业务费专项资金(D5000240144)