Al-2.5Cu-1.9Li-X合金的淬火敏感性及淬透性研究OA
Study on the Quenching Sensitivity and Hardenability of the Al-2.5Cu-1.9Li-X Alloy
本文采用等温保温方法及薄板叠层端淬并后续T8时效态强度测试方法,研究了Al-2.5Cu-1.9Li-X合金的淬火敏感性及淬透性.结果表明:固溶处理后于350~380 ℃等温保温不同时间时合金脱溶析出速率较快,相应合金的电导率上升速率较快,后续T6时效时析出的T1相明显减少,硬度降低速率较快;在此基础上,建立了该合金的C曲线,其"鼻尖"温度约为380 ℃,"鼻尖"温度附近5%转变量的孕育期为5.5s,远高于2195铝锂合金.薄板叠层端淬并T8时效后,随距淬火端距离的增加,合金强度逐渐降低.以相比淬火端强度下降10%的位置作为淬透层深度,则该铝锂合金的淬透层深度可达到80~90 mm,淬透性远优于高强2195铝锂合金.
The quenching sensitivity and hardenability of the Al-2.5Cu-1.9Li-X alloy were investigated by the interrupted quenching treatment and the method of testing the strength of laminated thin-sheet end-quenching after T8 aging treatment.After solution treatment,the number density of quenching precipitation phases is maximum in the alloys subjected to isothermal annealing at 350 to 380℃,and the electrical conductivity is the highest.Subsequent T6 aging results in a significant reduction of T1(Al2CuLi)precipitates and a rapid decrease in hardness.Based on these results,the C-curve of the alloy is established,and the"nose tip"temperature is approximately 380℃.The incubation period for 5%transformation near the nose temperature is 5.5 s,which is much higher than that of the 2195 Al-Li alloy.Furthermore,after laminated thin-sheet end-quenching and T8 aging,the strength gradually decreases with increasing distance from the quenched end.Taking a 10%decrease in strength relative to that at the quenched end as the depth of hardenability,the quenching depth of the Al-Li alloy reaches 80 to 90 mm,indicating a much better hardenability than that of the high-strength 2195 Al-Li alloy.
李劲风;曾广俊;刘添乐;马鹏程;陈永来
中南大学材料科学与工程学院,长沙 410083中南大学材料科学与工程学院,长沙 410083中南大学材料科学与工程学院,长沙 410083航天材料及工艺研究所,北京 100076航天材料及工艺研究所,北京 100076
矿业与冶金
铝锂合金淬火敏感性淬透性微观组织
Al-Li alloyQuenching sensitivityHardenabilityMicrostructure
《宇航材料工艺》 2026 (4)
93-100,8
评论