随着航空航天及超高速飞行器等高端装备的快速发展,对结构陶瓷材料在复杂摩擦磨损环境下的承载能力、耐磨性能及服役稳定性提出了更高要求,Si3N4这类结构陶瓷因其优异的综合性能被广泛应用,但其在严苛复杂服役环境下仍易发生疲劳开裂及磨损失效,失效原因与材料内部的显微组织结构密切相关.本文采用X射线衍射、扫描电子显微镜环形背散射电子成像和透射电子显微分析等多尺度表征手段,研究了添加TiN对Al2O3-Y2O3助剂体系无压烧结Si3N4陶瓷显微组织的影响及其作用机理.结果表明,添加TiN能够显著改善Al2O3-Y2O3体系液相烧结温度不均匀、驱动力不足所导致的晶粒粗大与孔隙残留问题,还可促进β-SiAlON固溶相的形成.TiN既作为异质位点提高β-Si3N4的形核密度,又因其高热稳定性对晶界起钉扎作用,可显著细化烧结产物β-Si3N4的晶粒组织并提高组织致密度;由于TiN与Si3N4具有较小的晶格错配度,可促进(30(3)0)Si3N4//(200)TiN及(0001)Si3N4//(011)TiN半共格界面的形成,从而改变氮化硅的磨损方式,减轻磨粒磨损与脆性剥落行为,提高氮化硅整体的耐磨性.

[Background and purposes]The rapid advancement of modern aerospace vehicles,hypersonic aircraft and high-tech equipment has raised higher demands on structural ceramic materials for load-bearing capacity,wear resistance and stability under complex friction and wear conditions.Si3N4 has been widely used due to its excellent properties.However,they are still prone to fatigue cracking and wear failures under severe operating conditions.These failures are closely related to the materials microstructure.In this study,Si3N4 ceramics with different contents of TiN were prepared by using pressureless sintering,with Al2O3-Y2O3 as sintering additives.The effects of TiN content on phase composition,lattice parameters,grain structure and interfacial structure of silicon nitride ceramics were systematically examined,thus providing experimental evidence for the design and performance optimization of Si3N4. [Methods]Si3N4 ceramics were prepared by using pressureless sintering with α-Si3N4 as the main raw material.Al2O3 and Y2O3 were used as sintering additives at contents of 3.0 wt.%and 6.0 wt.%,respectively,while 5.0 wt%β-Si3N4 seed crystals were introduced to promote the phase transformation during sintering.The raw powders were ball-milled with absolute ethanol as solvent.After drying,the ceramic powder mixture was ground and sieved through 200-mesh screen to ensure uniform particle size distribution.50 g powder was put into a 40-mm-diameter mold and compressed using a two-step compression process.The raw powder was first pre-pressed at 30 MPa for 3 min to form a preform,which was then placed into a 20 mm-diameter mold for cold isostatic pressing at 200 MPa for 5 min,yielding ceramic green bodies with uniform thickness and consistent dimensions.The compacted samples were placed in pressureless sintering furnace,purged three times with high-purity nitrogen and then sintered at 0.1 MPa high-purity N2,using two-step heating to 1600 ℃ at 10 ℃·min-1 and holding for 2 h,followed by heating to 1800 ℃ at the same rate and holding for 8 h to achieve densification of Si3N4 ceramics.After sintering,the samples were furnace-cooled to room temperature.The sample density was measured by using Archimedes method.XRD was used to analyze the phase composition and lattice parameters of Si3N4.The grain structure,phase and elemental distribution were characterized by using CBS,SEM and EDS.The Si3N4/TiN interfaces were characterized by using aberration-corrected TEM to analyze their interface and lattice mismatch. [Results]The addition of TiN addition improved densification of the pressureless-sintered Si3N4 with the Al2O3-Y2O3 sintering-aid system,increased relative density and reduced residual porosity and microstructural inhomogeneity,which are caused by insufficient driving force during the liquid-phase sintering.With increasing content of TiN,the grain-refinement effect becomes more pronounced.TiN promoted the diffusion and solid-solution reaction of Al and O in Si3N4,thereby facilitating the formation ofβ-SiAlON solid solution,effectively consuming free oxygen and suppressing the formation of the harmful Si2N2O phase.According to the high-resolution TEM results,TiN refined the Si3N4 grain through two primary mechanisms.Firstly,TiN particles,which have a high melting point of 2930-2950 ℃,pinned the Si3N4 grain boundaries and effectively suppressed grain growth.Secondly,low lattice mismatch,between TiN crystal planes[such as(200)and(011)]and Si3N4 crystal planes[such as(3030)and(0001)],provideed conditions for the heterogeneous nucleation of β-Si3N4,increasing the nucleation density of β-Si3N4.The resultant Si3N4 grains form stable semi-coherent interfaces with TiN.Due to grain refinement and stable interfacial structure,the worn surfaces become smoother,the wear tracks become shallower and brittle spalling is effectively suppressed,resulting in a marked improvement in wear resistance of the Si3N4 ceramics. [Conclusions]To address the problems of insufficient densification,coarse grains and limited wear resistance of pressureless-sintered Si3N4 ceramics prepared with conventional Al2O3-Y2O3 sintering additives,TiN with varying content was used.The effect phase composition,microstructure and interfacial structure was systematically studied.The addition of TiN addition significantly increased the densification of the material and suppressed the formation of the harmful Si2N2O.The addition of TiN also enhanced the diffusion and solid solution of Al and O within Si3N4,thereby facilitating the formation of the β-SiAlON solid solution.Furthermore,the addition of TiN effectively refined the Si3N4 grains and promoted the formation of stable semi-coherent interfaces by enhancing heterogeneous nucleation and grain boundary pinning.As a result,the worn surfaces of the Si3N4 ceramics became smoother,the wear tracks became shallower,the brittle spalling was significantly reduced and the wear resistance was markedly increased.

邓超;陈松;张伟儒;林燕;林家源;王卫国

福建理工大学材料科学与工程学院,福建 福州 350118福建理工大学材料科学与工程学院,福建 福州 350118中材高新氮化物陶瓷有限公司,山东淄博 255022||中材高新材料股份有限公司,北京 100021福建理工大学材料科学与工程学院,福建 福州 350118福建理工大学材料科学与工程学院,福建 福州 350118福建理工大学材料科学与工程学院,福建 福州 350118

化学化工

氮化硅陶瓷异质形核钉扎过渡金属化合物显微组织

silicon nitride ceramicsheterogeneous nucleationpinningtransition metal compoundsmicrostructure