首页|期刊导航|市政技术|基于MEPDG的橡胶沥青长寿命路面结构设计

基于MEPDG的橡胶沥青长寿命路面结构设计OA

Long-life Pavement Structure Design of Rubberized Asphalt Based on MEPDG

中文摘要英文摘要

结合路面结构、材料特性与应用环境,提出了基于MEPDG疲劳模型的橡胶沥青长寿命路面材料-结构一体化设计方法.基于橡胶沥青混合料疲劳试验数据校准MEPDG疲劳模型,结果表明,基于疲劳试验数据校准后的AC-13、AC-20级配以及通用级配模型,相关性达0.82.采用校准后的MEPDG疲劳模型分析了22种橡胶沥青长寿命路面结构.结合河北省冬季寒冷干燥、夏季炎热多雨、降水集中且季节性温湿变化显著的气候特征与交通条件,半刚性基层橡胶沥青路面推荐结构为:4 cm橡胶沥青混凝土上面层+8 cm橡胶沥青混凝土中面层+12 cm橡胶沥青混凝土下面层+(18+18+18)cm或(20+20+20)cm水泥稳定碎石基层,各橡胶沥青混凝土层最佳胶粉掺量为50%;全厚式橡胶沥青路面推荐结构为4 cm橡胶沥青混凝土上面层+10 cm橡胶沥青混凝土中面层+11 cm橡胶沥青混凝土下面层+11 cm橡胶沥青混凝土基层+18 cm级配碎石底基层,各橡胶沥青混凝土层最佳胶粉掺量为40%.选取橡胶沥青层永久变形量、橡胶沥青混合料层层底弯拉应变、半刚性基层层底最大拉应力、路基顶面竖向压应变、结构性车辙5个路面结构设计指标对上述2种结构进行验算,并通过校准后的疲劳模型反推临界应变以验证橡胶沥青混合料的疲劳寿命,结果均满足要求.该研究成果可为橡胶沥青长寿命路面设计提供可靠理论支撑.

Combining pavement structure,material properties and service environment,this paper proposes an inte-grated material-structure design method for long-life rubberized asphalt pavement based on the MEPDG fatigue model.The MEPDG fatigue model is calibrated with fatigue test data of rubberized asphalt mixtures.The results show that the correlation coefficient reaches 0.82 for AC-13,AC-20 gradations and the generic gradation model after calibration using fatigue test data.Twenty-two long-life rubberized asphalt pavement structures are analyzed using the calibrated MEPDG fatigue model.Considering the climatic features of Hebei Province,i.e.,cold and dry winters,hot and rainy summers,concentrated precipitation and prominent seasonal temperature-humidity variations,as well as local traffic conditions,the recommended semi-rigid base rubberized asphalt pavement structure is as follows:4 cm rubberized asphalt concrete surface course+8 cm rubberized asphalt concrete intermediate course+12 cm rubber-ized asphalt concrete lower course+(18+18+18)cm or(20+20+20)cm cement-stabilized macadam base.The op-timal crumb rubber content for each rubberized asphalt concrete layer is 50%.For the full-depth rubberized asphalt pavement,the recommended structure is 4 cm rubberized asphalt concrete surface course+10 cm rubberized asphalt concrete intermediate course+11 cm rubberized asphalt concrete lower course+11 cm rubberized asphalt concrete base+18 cm graded crushed stone subbase.The optimal crumb rubber content for each rubberized asphalt concrete layer is 40%.Five structural design indices,namely permanent deformation of rubberized asphalt layers,flexural-tensile strain at the bottom of rubberized asphalt mixture layers,maximum tensile stress at the bottom of semi-rigid base,vertical compressive strain on subgrade top surface,and structural rutting,are adopted to check the two pro-posed structures.The critical strains are back-calculated by the calibrated fatigue model to verify the fatigue life of rubberized asphalt mixtures,and all indices meet the specification requirements.The research outcomes can provide reliable theoretical support for the design of long-life rubberized asphalt pavements.

喻光勇;刘智慧;于华洋;樊凯德

西藏自治区林芝公路事业发展和应急保障中心,西藏自治区林芝 860004西藏自治区交通运输综合行政执法总队,西藏自治区拉萨 850030华南理工大学土木与交通学院,广东 广州 510641华南理工大学土木与交通学院,广东 广州 510641

交通工程

疲劳模型MEPDG橡胶沥青路面长寿命路面路面结构设计指标模型验证

fatigue modelMEPDGrubberized asphalt pavementlong-life pavementpavement structural design indexmodel verification

《市政技术》 2026 (9)

89-105,17

国家自然科学基金项目(52178426)

10.19922/j.1009-7767.2026.09.089