中文摘要英文摘要

基于机械合金化制备的 Cu-Sn-Bi 过饱和固溶体粉末,系统研究了其烧结工艺、相析出行为、微观组织演变及力学性能,并通过 Bi 和 Sn 含量对比实验,分别明确了 Bi 对微观组织的调控规律和 Sn 固溶强化的作用.结果表明:Cu-10%Sn-5%Bi 球磨 40 h 后形成 Cu(Sn,Bi)过饱和固溶体;烧结过程中 Sn 始终保持固溶态,Bi 在约 400℃开始从过饱和固溶体中脱溶析出,形成弥散分布的游离 Bi 相,确定最佳烧结温度为 750℃.微观组织随 Bi 含量增加而演变:3%时 Bi 相少量弥散,5%时呈均匀细小颗粒,7%时局部连通并割裂基体.Cu-10%Sn-5%Bi 合金在 750℃烧结后致密度为 92.8%,硬度 116 HV,拉伸强度 164.4 MPa.Sn 含量对比实验表明,高 Sn 合金具有更低的摩擦系数和更平整的磨损表面.

Based on the Cu-Sn-Bi supersaturated solid solution powders prepared by mechanical alloying,this study systematically investigates the sintering process,phase precipitation behavior,microstructural evolution,and mechanical properties.Through comparative experiments with varying Bi and Sn contents,the regulatory effect of Bi on the microstructure and the role of Sn solid-solution strengthening are clarified.The results show that after 40 h of ball milling,the Cu-10%Sn-5%Bi powder forms a Cu(Sn,Bi)supersaturated solid solution.During sintering,Sn remains in a solid-solution state,while Bi precipitates from the supersaturated solid solution at about 400℃,forming a finely dispersed free Bi phase.The optimal sintering temperature is 750℃.With increasing Bi content,the microstructure evolves as follows:at 3%Bi,the Bi phase is finely and sparsely dispersed;at 5%Bi,it distributes uniformly as fine particles;at 7%Bi,it becomes locally interconnected and splits the matrix.After sintering at 750℃,the Cu-10%Sn-5%Bi alloy achieves a relative density of 92.8%,a hardness of 116 HV,and a tensile strength of 164.4 MPa.Sn content comparison experiments show that the higher Sn alloy exhibits a lower friction coefficient and a smoother worn surface.

何秋梅;侯建明

广东水利电力职业技术学院 智能制造学院,广东 广州 510635广东水利电力职业技术学院 智能制造学院,广东 广州 510635

通用工业技术

机械合金化Cu-Sn-Bi过饱和固溶体烧结行为力学性能摩擦学性能

mechanical alloyingCu-Sn-Bisupersaturated solid solutionsintering behaviormechanical propertiestribological performance

《有色金属材料与工程》 2026 (3)

1-6,6

10.13258/j.cnki.nmme.20260609001

评论