先进高强钢热轧态氧化铁皮还原退火行为OA
Reduction Annealing Behavior of As-Rolled Scale on Advanced High-Strength Steel
针对热轧免酸洗高强钢及免酸洗还原退火技术在工业化应用中的核心问题,通过模拟退火试验研究了热轧态先进高强钢表面氧化铁皮的还原行为.在30%H2、70%N2(体积分数)的混合还原气氛中,于500~1 100 ℃范围内进行等温还原试验.结果表明:氧化铁皮还原动力学过程呈现明显的三阶段温度依赖特征,500~700 ℃时以原子形核与长大为控速步骤,还原产物为多孔铁;800~1 100 ℃时控速机制转变为相界反应和扩散,还原产物为致密铁;700 ℃时出现还原低谷,氧化铁皮在该温度下完成由多孔结构向致密结构的转变;当温度达到800 ℃及以上时,基体中发生内氧化,内氧化物形态随温度升高由条状逐渐演变为点状.
To address the core issues in the industrial application of pickling-free hot-rolled high-strength steel and pickling-free reduction annealing technology,the reduction behavior of the scale on as-rolled advanced high-strength steel was investigated through simulated annealing experiments.Isothermal reduction experiments were conducted in a mixed reducing atmosphere of 30%H2 and 70%N2(volume fraction)over a temperature range of 500~1 100 ℃.The results demonstrated that the reduction kinetics of the scale exhibited a distinct three-stage temperature-dependent behavior.In the range of 500~700 ℃,atomic nucleation and growth were the rate-controlling steps,yielding porous iron as the reduction product.In the range of 800~1 100 ℃,the rate-controlling mechanism shifted to phase-boundary reaction and diffusion,resulting in dense iron.A reduction trough was observed at 700 ℃,where the scale underwent a transition from a porous to a dense structure.When the temperature reached 800 ℃ or above,internal oxidation occurred in the substrate,and the morphology of the internal oxides gradually evolved from strip-like to dot-like with increasing temperature.
孙彬;张苇豪
沈阳大学机械工程学院,辽宁 沈阳 110044沈阳大学机械工程学院,辽宁 沈阳 110044
矿业与冶金
热轧态先进高强钢,氧化铁皮高温氧化还原退火内氧化
as-rolled advanced high-strength steelscalehigh-temperature oxidationreduction annealinginternal oxidation
《沈阳大学学报(自然科学版)》 2026 (4)
263-270,封2,封3,10
"兴辽英才计划"青年拔尖人才项目(XLYC2203082).
评论