废旧涤棉纤维吸声复合材料的制备及性能OA

Preparation and properties of sound absorption composites from waste polyester/cotton fibers

中文摘要英文摘要

为解决废旧涤棉纤维回收难分离和噪声污染的问题,以废旧涤棉纤维和乙烯-乙酸乙烯共聚物为原料,利用混炼-热压发泡技术,通过单因素实验制备1 cm厚度的材料,探究偶氮二甲酰胺发泡剂(AC)含量、废旧涤棉纤维质量分数、热压压强、热压时间以及热压温度对材料吸声性能的影响.对各材料的平均吸声系数和降噪系数进行综合分析,确定最优工艺参数:发泡剂AC质量分数4%,废旧涤棉纤维质量分数10.00%,热压压强3 MPa,热压时间15 min,热压温度190 ℃.在最优工艺条件下,多孔复合吸声材料的最高吸声系数达到0.81,平均值达到0.32,降噪系数0.25,吸声性能等级达到Ⅳ级.

To address the difficulties in separating waste polyester/cotton fibers and the problem of noise pollution,waste polyester/cotton fibers and ethylene-vinyl acetate copolymer were used as raw materials,and a mixing-calendering and hot-press foaming technique was adopted.Materials with a thickness of 1 cm were prepared by single-factor experiments,and the effects of azodicarbonamide(AC)blowing agent content,waste polyester/cotton fibers mass fraction,hot-press pressure,hot-press time,and hot-press temperature on the sound absorption properties of the materials were investigated.The average sound absorption coefficients and noise reduction coefficients of each material were calculated for comprehensive analysis,and the optimal process parameters were determined as follows:AC blowing agent content of 4%,waste polyester/cotton fibers mass fraction of 10.00%,hot-press pressure of 3 MPa,hot-press time of 15 min,and hot-press temperature of 190℃.Under the optimal process conditions,the maximum sound absorption coefficient of the porous composite sound-absorbing material was found to reach 0.81,the average value was measured to be 0.32,the noise reduction coefficient was calculated as 0.25,and the sound absorption performance grade was evaluated to be Grade Ⅳ.

赵懿平;胡大仟;吕丽华

大连工业大学纺织与材料工程学院,辽宁大连 116034大连工业大学纺织与材料工程学院,辽宁大连 116034大连工业大学纺织与材料工程学院,辽宁大连 116034

轻工纺织

废旧涤棉吸声材料混炼-热压发泡多孔吸声

waste polyester cottonsound absorbing materialmixing-hot press foamingporous sound absorption

《大连工业大学学报》 2026 (4)

279-284,6

大连市科技创新基金项目(2019J12SN71).

10.19670/j.cnki.dlgydxxb.2026.0408

评论