深冷换热器铜/不锈钢异种金属焊接工艺与评定方案设计OA
Design of a Welding Process Scheme and Qualification Scheme for Cop-per/Stainless-Steel Dissimilar-Metal Tube-to-Tubesheet Joints in Cryo-genic Heat Exchangers
针对深冷(液氮-196℃)工况下铜管-不锈钢管板异种焊接接头的可靠性问题,设计了焊接工艺方案及配套的焊接工艺评定(WPQR)方案.针对液态铜沿奥氏体晶界渗透致裂及Fe-Cu低熔点共晶热裂难题,采用"304管板镍基堆焊过渡层+ERNiCr-3镍基焊丝管子-管板角焊+焊后贴胀"复合工艺,以镍与铜、铁无限固溶避免Fe-Cu低熔点共晶热裂,以堆焊层隔离铜液与不锈钢,并辅以铜侧预热、电弧偏铜侧及脉冲控温克服未熔合、控制Fe稀释.依据NB/T 47014-2023设计涵盖外观、无损检测、宏观金相、力学、低温冲击与致密性的系统评定方案,明确试件制备、测试方法、合格判据及各项设计目标值/文献预测值.上述量值均为设计目标值/预测值、非本研究实测,须经评定试件实测验证后方可作为正式合格结论.研究为该类铜/不锈钢管子-管板异种接头的工艺设计与评定方案制定提供工程化参考.
To address the reliability of copper-tube/stainless-steel-tubesheet dissimilar-metal joints under cryogenic service(liquid nitrogen,-196℃),a welding process scheme and a matching welding procedure qualification(WPQR)scheme are proposed.Against liquid-copper penetration cracking along austenitic grain boundaries and low-melting Fe-Cu eutectic hot cracking,a composite scheme is adopted:a nickel-based buttering layer on the SUS304 tubesheet,an ERNiCr-3 tube-to-tubesheet fillet weld,and post-weld light expansion;the complete Ni-Cu-Fe solid solubility avoids low-melting eutectics,the buttering layer isolates liquid copper from the steel,and copper-side preheating,an arc offset toward the copper and pulsed control overcome lack of fusion and confine Fe dilution.A systematic qualification scheme per NB/T 47014-2023(appear-ance,PT,macro-metallography,mechanics,low-temperature impact,tightness)defines specimens,methods,criteria and design-target/predicted values(helium leak rate≤1×10-9 Pa·m3/s;shear/tensile strength 230-260 MPa,fracture in the copper base metal;no obvious ductile-brittle transition at-196℃).All values herein are design targets/predictions rather than mea-sured results and require qualification testing for confirmation.The work provides an engineering-oriented reference for pro-cess design and qualification-scheme formulation of such joints.
吴磊;种彪;李新银;李伟
枣庄市特种设备检验研究院(市特种设备安全技术检查中心、市产品质量监督检验所),山东 枣庄 277101枣庄市特种设备检验研究院(市特种设备安全技术检查中心、市产品质量监督检验所),山东 枣庄 277101山东密友机械有限公司,山东 枣庄 277500山东密友机械有限公司,山东 枣庄 277500
矿业与冶金
深冷换热器铜/不锈钢异种焊接镍基过渡层ERNiCr-3管子-管板角焊缝焊接工艺评定
cryogenic heat exchangercopper/stainless-steel dissimilar weldingnickel-based buttering layerERNiCr-3tube-to-tubesheet fillet weldwelding procedure qualification
《电焊机》 2026 (9)
74-80,121,8