Cr-Ni-Mn成分调控对316LMn型不锈钢药芯焊丝熔敷金属低温韧性的影响OA

Effect of Cr-Ni-Mn Composition Regulation on the Low-Temperature Tough-ness of Deposited Metal from 316LMn-Type Stainless Steel Flux-Cored Wire

中文摘要英文摘要

针对316LMn型不锈钢药芯焊丝熔敷金属在-196℃低温条件下冲击韧性差异的问题,采用Cr-Ni-Mn三因素三水平正交试验设计方法制备不同成分组合的熔敷金属,结合力学性能测试、极差分析、方差分析、显微组织表征及断口分析,研究合金元素及其交互作用对熔敷金属低温韧性和断裂行为的影响规律.结果表明,极差分析显示Ni元素对-196℃冲击功影响最大(R=26.67),其次为Mn(R=14.00)和Cr(R=7.33);方差分析表明Ni元素影响最为显著(F=291.35,P=0.000 4),Mn元素达到显著水平(F=79.14,P=0.003),同时Cr-Ni和Cr-Mn交互作用对低温冲击性能具有显著影响.综合分析确定理论优化成分组合为Cr 22 wt.%、Ni 20 wt.%、Mn 7 wt.%.在成分调控作用下,熔敷金属凝固组织及相组成发生明显变化,进而导致不同试样间低温韧性差异,WM-4试样主要由细小胞状晶和等轴晶组成;WM-6试样则形成粗大柱状晶及局部δ-铁素体区域,并伴随较多Mn-Si-O系复合夹杂物.冲击断口分析表明,WM-4以密集韧窝断裂为主,表现出良好的塑性变形能力;WM-6呈现韧性断裂与准解理断裂共存的混合断裂特征,其中高Cr/低Ni特征δ-铁素体区域易形成准解理平台及穿晶二次裂纹,是导致低温冲击韧性下降的主要原因,夹杂物作为局部裂纹萌生位置,对低温断裂行为具有辅助作用.研究结果可为超低温奥氏体不锈钢焊接材料的成分精准设计提供依据.

The low-temperature impact toughness discrepancy of deposited metals from 316LMn-type stainless steel flux-cored wires at-196℃was investigated.A Cr-Ni-Mn three-factor and three-level orthogonal experimental design was em-ployed to prepare deposited metals with different alloy compositions.Combined with mechanical property testing,range analysis,analysis of variance(ANOVA),microstructural characterization,and fracture analysis,the effects of alloying ele-ments and their interactions on the low-temperature toughness and fracture behavior of deposited metals were systematically analyzed.The results indicated that Ni exhibited the greatest influence on the impact toughness at-196℃,with a range value of 26.67,followed by Mn(14.00)and Cr(7.33).ANOVA results demonstrated that Ni had the most significant effect(F=291.35,P=0.0004),while Mn also showed a significant influence(F=79.14,P=0.0030).Furthermore,the Cr-Ni and Cr-Mn interactions were found to significantly affect the low-temperature impact properties.The theoretical optimized composi-tion was determined as Cr 22 wt.%,Ni 20 wt.%,and Mn 7 wt.%.The regulation of alloy composition resulted in significant changes in the solidification microstructure and phase constitution of the deposited metals,leading to variations in low-temperature toughness among different specimens.The WM-4 specimen was mainly composed of fine,uniformly distrib-uted cellular crystals and equiaxed grains,whereas the WM-6 specimen exhibited coarse columnar grains,localized δ-ferrite regions,and abundant Mn-Si-O complex inclusions.Fracture analysis revealed that the WM-4 specimen exhibited a typical ductile fracture dominated by dense dimples,indicating superior plastic deformation capability.In contrast,the WM-6 speci-men showed a mixed fracture mode combining ductile fracture and quasi-cleavage fracture.The high-Cr/low-Ni δ-ferrite re-gions facilitated the formation of quasi-cleavage facets and transgranular secondary cracks,which were identified as the pri-mary factors responsible for the deterioration of low-temperature impact toughness.Meanwhile,inclusions acted as preferen-tial sites for local crack initiation and contributed to the low-temperature fracture behavior.The findings provide a basis for the precise compostion design of austentic stainless steel welding material for cryogentic service.

李彦哲;徐锴;沈海琴;喻朝飞;周璐宽;念林哲

哈焊所华通(常州)焊业股份有限公司,江苏 常州 213102||中国机械总院集团哈尔滨焊接研究所有限公司,黑龙江 哈尔滨 150028哈焊所华通(常州)焊业股份有限公司,江苏 常州 213102||中国机械总院集团哈尔滨焊接研究所有限公司,黑龙江 哈尔滨 150028中车戚墅堰机车有限公司,江苏 常州 213011哈焊所华通(常州)焊业股份有限公司,江苏 常州 213102哈焊所华通(常州)焊业股份有限公司,江苏 常州 213102哈焊所华通(常州)焊业股份有限公司,江苏 常州 213102

矿业与冶金

316LMn不锈钢药芯焊丝合金元素低温冲击韧性凝固组织断裂行为

316LMn stainless steelflux-cored wirealloying elementslow-temperature impact toughnesssolidification mi-crostructurefracture behavior

《电焊机》 2026 (9)

66-73,8

10.7512/j.issn.1001-2303.2026.09.07