首页|期刊导航|电焊机|高熵复合钎料钎焊Si3N4/42CrMo异质接头焊缝组织调控与性能提升机制

高熵复合钎料钎焊Si3N4/42CrMo异质接头焊缝组织调控与性能提升机制OA

Microstructure Control and Strengthening Mechanisms of Si3N4/42CrMo Dissimilar Joints Brazed with a High-Entropy Composite Filler Alloy

中文摘要英文摘要

本研究首次采用FeCoNiCr高熵合金颗粒增强AgCuTi活性钎料,在880℃下保温10 min,实现了Si3N4陶瓷与42CrMo钢的可靠钎焊连接.接头在Si3N4界面处形成由TiN和Ti5Si3组成的连续反应层,钎缝内部主要由富Ag固溶体、富Cu固溶体、Cu-Ti相、FCC结构FeCoNiCr相、富Cr相及Ti(CuFeCoNi)x相构成,靠近42CrMo钢一侧则形成Cu-Ti和Fe2Ti反应产物.FeCoNiCr颗粒的加入改变了Ti元素在钎缝中的扩散、溶解与反应行为,促进多组元反应相形成,并削弱粗大连续Cu-Ti脆性相的生成倾向.适量添加可细化钎缝组织,使反应产物由连续或块状分布转变为细小弥散分布,改善界面应力传递并缓解陶瓷与金属之间的热膨胀失配;添加过量则会降低钎料流动性和界面润湿能力,导致FCC颗粒及反应产物局部团聚,形成新的应力集中区域.当FeCoNiCr含量为0.5 wt.%时,接头剪切强度达到约136 MPa,较未添加时提高64%,断裂模式由以陶瓷侧脆性断裂为主转变为陶瓷、界面及钎缝共同参与的混合断裂,从而提高接头整体承载稳定性.

In this study,FeCoNiCr high-entropy alloy particles were employed for the first time to reinforce an AgCuTi ac-tive brazing filler,enabling reliable brazing of Si3N4 ceramic to 42CrMo steel at 880℃for 10 min.A continuous reaction layer composed of TiN and Ti5Si3 formed at the Si3N4 interface.The brazing seam mainly consisted of Ag-rich and Cu-rich solid solutions,Cu-Ti phases,FCC-structured FeCoNiCr particles,Cr-rich phases,and Ti(CuFeCoNi)ₓ phases,while Cu-Ti and Fe₂Ti reaction products formed adjacent to the 42CrMo steel.The addition of FeCoNiCr particles altered the diffusion,dissolution,and reaction behavior of active Ti in the brazing seam,promoted the formation of multicomponent reaction phases,and suppressed the formation of coarse and continuous brittle Cu-Ti phases.An appropriate addition refined the brazing-seam microstructure and transformed the reaction products from continuous or blocky morphologies into fine and dispersed phases,thereby improving interfacial stress transfer and alleviating the thermal-expansion mismatch between the ceramic and metal.Excessive addition,however,reduced the fluidity and interfacial wettability of the filler,resulting in local agglomeration of FCC particles and reaction products and creating additional stress-concentration regions.At a FeCoNiCr content of 0.5 wt.%,the joint achieved a maximum shear strength of approximately 136 MPa,representing a 64%increase compared with the joint without FeCoNiCr.Meanwhile,the fracture mode changed from predominantly brittle fracture on the ceramic side to mixed fracture involving the ceramic,interface,and brazing seam,thereby improving the overall load-bearing stability of the joint.

张晓航;盛兰兵;尹东坤;沈宇;佘春;沈元勋

中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001

矿业与冶金

Si3N4陶瓷异种材料钎焊高熵合金力学性能界面组织

Si3N4 ceramicheterogeneous material brazinghigh-entropy alloymechanical propertiesinterfacial microstructure

《电焊机》 2026 (9)

46-57,12

10.7512/j.issn.1001-2303.2026.09.05