针对海洋工程、工程机械等领域中厚板传统多层多道焊坡口加工量大、焊材消耗高及单道全熔透焊接中背面成形稳定性差等问题,提出并开发了脉冲激光+CMT电弧复合热源高效焊接工艺.以10 mm厚Q235B钢板为研究对象,通过分析热源引导模式、光丝间距及激光脉冲参数等工艺条件对电弧稳定性、焊缝熔透状态和焊缝成形的影响.结果表明,激光引导模式能够减小电弧电压及熔滴过渡周期的波动;在连续激光条件下,熔透状态易在未熔透与背面驼峰之间突变;脉冲激光可以有效调节激光瞬时穿透能力,避免在焊透的条件下出现驼峰缺陷,其中占空比对背面成形的影响比脉冲频率更为显著;通过参数优化实现了在不开坡口、无背面辅助成形条件下良好的单道焊双面成形.所得接头拉伸试样断裂于母材,抗拉强度和断后延伸率分别为478.4 MPa和22.9%;焊缝中心及熔合区室温冲击吸收功分别为55.9 J和91.6 J,接头未出现明显软化区,综合力学性能良好.新开发的工艺应用于壁厚10 mm液压缸筒的焊接,相较传统多层多道MAG焊接效率提高约80%,焊丝消耗减少约84%,圆度和同心度偏差控制在0.1 mm以内,为中厚板结构的高效、低耗制造提供了新的技术途径.

To address the extensive groove preparation and high filler metal consumption associated with conventional multi-pass welding of medium-thick low-carbon steel plates,as well as the poor stability of the back-weld appearance during one-pass full-penetration welding,a pulsed laser-cold metal transfer(CMT)arc hybrid welding process was proposed.10 mm-thick Q235B steel plates were used to investigate the effects of the heat-source leading mode,laser-arc distance,and laser pulse parameters on arc stability,weld penetration,and weld appearance.A Box-Behnken design was further employed to optimize the pulse frequency and duty cycle of the laser beam.The results showed that the laser-leading mode reduced fluc-tuations in arc voltage and droplet-transfer period.If the continuous laser was used,the weld penetration state changed abruptly between incomplete penetration and back humping weld.While the pulsed laser can provide additional control of the instantaneous penetration capability to inhibit the formation of back humping weld,the duty cycle had a more significant effect on back-weld appearance than the pulse frequency.At the optimized parameter combination of a pulse frequency of 112 Hz and a duty cycle of 91%,sound one-pass welding with back-formation was achieved without groove or back-forming assistance.The tensile specimens fractured in the base metal,and the tensile strength and elongation were 478.4 MPa and 22.9%,respectively.The room-temperature impact energies at the weld center and fusion zone were 55.9 J and 91.6 J,respectively,and the joint exhibited good overall mechanical properties.The developed welding process was used to manufacture hydraulic cylinder barrels with a 10 mm wall thickness;the welding efficiency increased by approximately 80%,filler wire consumption decreased by approximately 84%,and the roundness and concentricity deviations were less than 0.1 mm.The developed welding process offers a new technical approach to highly efficient,low-energy welding of medium-thick steel structures.

樊祥辰;梁国栋;金鹏;秦国梁

山东大学 材料科学与工程学院,山东 济南 250061||山东省高等学校能源装备智能焊接校企产学研协同创新中心,山东 济南 250061山东大学 材料科学与工程学院,山东 济南 250061||山东省高等学校能源装备智能焊接校企产学研协同创新中心,山东 济南 250061山东大学 材料科学与工程学院,山东 济南 250061||山东省高等学校能源装备智能焊接校企产学研协同创新中心,山东 济南 250061山东大学 材料科学与工程学院,山东 济南 250061||山东省高等学校能源装备智能焊接校企产学研协同创新中心,山东 济南 250061

矿业与冶金

激光+CMT电弧复合焊中厚板单道焊双面成形脉冲激光高效焊接

laser+CMT arc hybrid weldingmedium-thick plateone-pass welding with back-formationpulsed laser weld-inghigh-efficiency welding

《电焊机》 2026 (9)

10-22,13

国家自然科学基金区域创新发展基金重点项目(U21A20129)

10.7512/j.issn.1001-2303.2026.09.02

评论