激光增材修复300M高强度钢的显微组织与力学性能OA
Microstructure and mechanical properties of laser additive manufacturing-repaired 300M high-strength steel
为了挖掘航空高强度钢构件修复技术的经济效益和科研价值,适配航空航天领域发展需求,采用激光增材修复技术对300M高强度钢基体裂纹进行修复.对修复试样的显微组织、元素分布、静态力学性能及断口形貌进行研究.结果表明,修复区组织自顶层向基体方向依次呈现贝氏体 → 马氏体+贝氏体 → 回火马氏体的梯度特征,热影响区组织主要为不均匀的马氏体,热处理后各区域均转变为均匀的回火马氏体和贝氏体混合组织.沉积态试样修复区硬度高于基体,但热影响区存在软化;沉积态拉伸试样抗拉和屈服强度低、塑性好,断口为准解理形貌,经合适热处理后强度大幅提高但塑性显著下降,断口转变为韧性断裂.
To tap into the ecohomic benefits and scientific research value of repair techonlogy for aerospace high-strength steel components and meet the development needs of aerospace field,laser additive manufacturing repair technology was employed to repair cracks in 300M high-strength steel substrates.The microstructure,element distribution,static mechanical properties,and fracture morphology of the repaired specimen were analyzed.Results indicate that the microstructure of the repair zone exhibits a gradient characteristic from the top layer to the substrate:Bainite → Martensite+Bainite → Tempered Martensite.The heat-affected zone primarily consists of non-uniform Martensite.After heat treatment,all regions transform into a uniform mixture of tempered Martensite and Bainite.The as-deposited specimen shows higher hardness in the repair zone compared to the substrate,but softening occurs in the heat-affected zone.The as-deposited tensile specimen demonstrates low tensile and yield strength,good plasticity and a quasi-cleavage fracture morphology.After appropriate heat treatment,the strength increases significantly,but plasticity decreases markedly,and the fracture mode transitions to ductile fracture.
李东洋;杨光;任宇航
沈阳航空航天大学 机电工程学院,沈阳 110136||石家庄海山实业发展总公司试飞站,石家庄 050208沈阳航空航天大学 机电工程学院,沈阳 110136||石家庄海山实业发展总公司试飞站,石家庄 050208沈阳航空航天大学 机电工程学院,沈阳 110136||石家庄海山实业发展总公司试飞站,石家庄 050208
矿业与冶金
激光增材修复技术300M高强度钢显微组织力学性能热处理
laser additive manufacturing repair technology300M high-strength steelmicrostructuremechanical propertiesheat treatment
《沈阳航空航天大学学报》 2026 (4)
47-56,10
国家重点研发计划项目(项目编号:2022YFE0122600).