Q390低合金高强结构钢厚板双丝MIG焊接试验研究OA
Experimental study on double-wire MIG welding of Q390 low-alloy high-strength structural steel thick plates
为提高Q390低合金高强结构钢的焊接效率和质量,提出对Q390钢厚板采用多层多道双丝焊接工艺,分为打底焊、填充焊1、填充焊2、盖面焊等4道.结果表明:多层多道双丝焊接不会改变母材的化学成分,但会促使钢板组织由柱状粗晶体向条状细晶转变,显著提升焊缝的硬度,且打底焊的硬度>填充焊的硬度>盖面焊的硬度;Q390钢厚钢板焊接接头力学性能优异,平均抗拉强度达到531.7MPa,平均屈服强度为338MPa,平均伸长率可达到21.2%.焊缝区域的焊接残余应力较大,垂直和平行于焊缝方向上的最大残余应力分别达到377MPa和351MPa,虽均未超过Q390钢母材的屈服强度,但仍建议对厚板双丝焊缝采取恰当的处理方式来减小焊后残余应力.
To improve the welding efficiency and quality of Q390 low-alloy high-strength structural steel,a multi-layer and multi pass double wire welding process is proposed for Q390 thick plates,which includes four stages:bottom welding,fill welding 1,fill welding 2,and cover welding.The results show that multi-layer and multi pass double wire welding does not change the chemical composition of the base material,but promotes the transformation of the steel plate structure from columnar coarse crystals to strip-shaped fine crystals,significantly improving the hardness of the weld seam,and the hardness of the base welding is greater than that of the filler welding and the hardness of the cover welding;The mechanical properties of Q390 thick steel plate welded joints are excellent,with an average tensile strength of 531.7MPa,an average yield strength of 338MPa,and an average elongation rate of 21.2%.The welding residual stress in the weld area is relatively high,with maximum residual stresses perpendicular and parallel to the weld direction reaching 377MPa and 351MPa,respectively.Although both do not exceed the yield strength of Q390 base metal,it is still recommended to adopt appropriate treatment methods for thick plate double wire welds to reduce post weld residual stress.
邓蕾;向高
武汉城市学院 湖北武汉 430000武汉城市学院 湖北武汉 430000
Q390低合金高强结构钢双丝焊接工艺接头力学性能焊接残余应力
Q390 low-alloy high-strength structural steeldouble wire welding processmechanical properties of jointswelding residual stress
《金属加工(热加工)》 2026 (9)
30-35,6