首页|期刊导航|金刚石与磨料磨具工程|Cf/SiC复合材料激光预制微沟槽对磨粒划擦去除机理的影响

Cf/SiC复合材料激光预制微沟槽对磨粒划擦去除机理的影响OA

Mechanism of abrasive scratching removal affected by laser prefabricated micro-grooves in Cf/SiC composite materials

中文摘要英文摘要

研究激光预制微沟槽对材料去除机理的影响,以提高Cf/SiC复合材料的加工效率.采用纳秒激光对工件表面进行微沟槽加工,并进行单颗磨粒划擦实验.通过改变划擦载荷,分析不同设定载荷下动态载荷和声发射信号的变化规律,结合显微镜观察划擦形貌,分析不同纤维方向下的材料去除行为与机理.结果表明,平行于纤维方向上的划痕边缘较整齐,有少许纤维剥离留下的凹坑;垂直于纤维方向上的划痕边缘则呈现参差不齐的纤维断裂和三角形的块状剥落.微沟槽的存在使沟槽附近材料出现下陷现象,微沟槽附近的垂直纤维呈三角形撕裂状.当载荷分别为2,4,6 N时,无微沟槽表面最大声发射信号的峰值频率分别为2 167,1 814,2 883 Hz;而激光预制微沟槽的存在使得声发射信号更加密集,当载荷分别为 2,4,6 N时,最大声发射信号的峰值频率分别为 4 190,8 736,5 052 Hz.结合形貌分析得出,材料整体以脆性去除为主,平行方向纤维以拉伸断裂为主,垂直方向纤维以剪切断裂和弯曲断裂为主.激光预制微沟槽对材料的去除机理有一定影响:沿垂直于纤维方向划擦时,产生的拉应力使边缘的纤维在被压头剪断前脱离基体;沿平行于纤维方向划擦时,边缘的纤维在更低的拉应力下脱离基体,以较长的断裂纤维形式去除.激光预制微沟槽使得压头可在相同载荷下引发更多的基体与材料损伤,使材料更容易去除.

Objectives:Cf/SiC composite material is a kind of material difficult to be machined,and laser assisted grinding is a kind of composite processing method that can effectively improve the machining efficiency.Methods:In this work,a single diamond abrasive grain is used to carry out the quasi-static scratch experiment,the acoustic emission signals have been analyzed under different loads,and material removal behavior and scratch removal mechanism have been analyzed by combining with SEM.The experimental material is a cube Cf/SiC composite material with a side length of 10 mm.The material surface is polished to reduce the impact of surface defects and roughness.The material is divided into two groups,one of which uses a laser to create micro-grooves on the surface.Micro-grooves shall be kept away from holes.Laser process parameters are power 20 W,scanning times 50 times and scanning speed 200 mm/s.In the scratch test,the constant load is set as 2,4,and 6 N respectively,and the scratch length is set as 5 mm.In the experiment,data collector is used to collect acoustic emission signal and force signal respectively.Scratch patterns are photographed using different micro-grooves after the experiment.Results:The results show that a large amount of chips are distributed on both sides of the scratch after the material surface is scratched by the diamond indenter.When the scratch direction is parallel to the fiber direction,the material is mainly subject to brittle removal.The scratch edge is relatively smooth without obvious damage.There is a small amount of carbon fiber peeling at the scratch edge,leaving a semicircular groove on the SiC matrix.When the scratch direction is vertical to the fiber direction,the material is mainly removed by brittleness,and there is uneven fiber fracture at the scratch edge.In the case of laser-ablated grooves,the difference between the morphology of scratches and the absence of laser-ablated grooves is mainly concentrated near the grooves.When the indenter is scribed into the groove,the matrix at the edge of the groove is sunken,and the matrix at the inlet is torn in a triangular shape.Different acoustic emission signals are generated under different loads.At 2,4,and 6 N,the maximum AE signals produced by the grooveless surface are 2 167,1 814,and 2 883 Hz,respectively.The maximum AE signals generated by the grooved surface are 4 190,8 736,and 5 052 Hz,respectively.The greater the load,the greater the acoustic emission signal produced,and the greater the acoustic emission signal produced by the grooved surface,the more dense the acoustic emission signal.The micro-groove makes the force signal have obvious fluctuation.Conclusions:Based on the acoustic emission signal and scratch morphology,the material removal mechanism is obtained.The fibers in two directions are removed in different ways.Brittleness removal is the main method for the whole material,tensile fracture is the main method for the fibers in parallel direction,and shear fracture and bending fracture are the main methods for the fibers in vertical direction.The removal mechanism of materials varies significantly with fibers in different directions,and laser prefabricated micro-grooves have a certain impact on the removal mechanism of materials.Laser prefabricated micro-grooves cause more damage to the indenter under the same load,making the material easier to remove.

黄心浩;吴重军

东华大学 机械工程学院,上海 201600东华大学 机械工程学院,上海 201600

机械制造

Cf/SiC单颗磨粒划擦声发射信号激光织构材料去除机理

Cf/SiCsingle grit scratchingacoustic emission signallaser texturingmaterial removal mechanism

《金刚石与磨料磨具工程》 2026 (4)

506-514,9

10.13394/j.cnki.jgszz.2024.0140

评论