扫描速度对电子束选区熔化制备Ni-Cu/金刚石复合材料微观组织及性能的影响OA
Effect of scanning speed on microstructure and properties of Ni-Cu/diamond composites prepared by electron beam selective melting
传统聚晶金刚石复合片(PDC)钻头胎体多采用烧结或铣削等工艺制备,存在制备流程烦琐且精度有限等缺点,目前已无法满足高效率的钻探需求.采用电子束选区熔化技术成功制备 PDC钻头体用Ni-Cu/金刚石复合材料,聚焦于该技术中关键工艺参数对材料制备的影响,系统研究电子束打印时的扫描速度对Ni-Cu/金刚石复合材料微观组织、抗弯强度和耐磨性等性能的影响规律.结果表明:随着扫描速度增大,打印后Ni-Cu/金刚石复合材料样品的致密度呈先上升后下降的趋势,扫描速度为4.75 m·s-1时达到最大值为94.4%;当扫描速度从4.50 m·s-1 增大至5.50 m·s-1 时,样品的抗弯强度和磨耗比均呈先增大后减小的趋势,在扫描速度为4.75 m·s-1时同时达到最大值,分别为142.2 MPa和0.63,此时制备出的Ni-Cu/金刚石复合材料具有最优的抗弯强度和耐磨性能.
Objectives:With the development of geological drilling towards the deep Earth and deep sea,the requirements for the matrix material of drill bits are becoming increasingly stringent.Traditional polycrystalline diamond compact(PDC)drill bit bodies are mainly prepared by sintering a hard phase and a binder phase.The current problem is that it is difficult to resist the strong impact brought by a large number of solid particles of rock chips and high pumping pressure in deep drilling.The drill bit body will be damaged prematurely due to excessive wear,causing the PDC drill teeth to prematurely fall off or break,which greatly reduces the service life of the drill bit.In addition,the traditional PDC drill bit bodies are mainly made by machining or high-temperature sintering using a mold,which has the disadvantages of a long preparation cycle,low efficiency and poor control of drill bit precision.Methods:In this paper,Ni-Cu alloy powder and diamond powder are used as raw materials to prepare Ni-Cu/diamond composites for a PDC drill bit matrix by electron beam selective melting(EBSM).Through microscopic characterization and mechanical property testing,the effect of scanning speed on the density,bending strength and wear resistance of the Ni-Cu/diamond composite is systematically investigated.Results:The results show that with the gradual increase of the scanning speed,the density,bending strength,and wear ratio of Ni-Cu/diamond composite samples after printing show a trend of first increasing and then gradually decreasing.When the scanning speed is 4.50 m·s-1,the scanning speed is low,and the heat input on the surface of the mixed raw materials is too large,which leads to the formation of defects and pores,so the performance of the Ni-Cu/diamond composite sample under this condition is poor.When the scanning speed is 4.75 m·s-1,the density,flexural strength and wear ratio reach the maximum values of 94.4%,142.2 MPa and 0.63,respectively,and the wear resistance of the sample reaches the optimal value.When the scanning speed is further increased to 5.50 m·s-1,part of the metal powder on the specimen surface is not sufficiently melted due to the excessive scanning speed,resulting in cracks and bonding defects appearing inside the specimen,so the specimen's performance shows a decreasing trend.Conclusions:Therefore,it can be concluded that the prepared Ni-Cu/diamond composites exhibit optimal bending strength and wear resistance when the electron beam scanning speed is 4.75 m·s-1.
李浩东;刘麦子;王一帆;范永刚;王聪
东北大学 冶金学院,沈阳 110819东北大学 冶金学院,沈阳 110819西安赛隆增材技术股份有限公司,西安 710018东北大学 冶金学院,沈阳 110819东北大学 冶金学院,沈阳 110819
化学化工
电子束选区熔化(EBSM)Ni-Cu/金刚石复合材料抗弯强度磨耗比
electron beam selective melting(EBSM)Ni-Cu/diamond compositesbending strengthwear ratio
《金刚石与磨料磨具工程》 2026 (4)
461-469,9
国家重点研发计划(2021YFB3701800)国家自然科学基金(52104360,52374367).
评论