单脉冲能量对激光清洗7B04铝合金锈蚀层的影响OA
Effect of Single Pulse Energy on Laser Cleaning of Corrosion Layer of 7B04 Aluminum Alloy
7B04铝合金因其密度低、比强度高的优异性能,被广泛应用于飞机结构.但在严酷的服役环境下,其表面易发生腐蚀,进而影响飞机的使用性能.为获得更优的除锈方法并确定激光清洗的优化参数,本文结合温度场仿真与试验,对激光除锈与机械打磨除锈进行了对比研究.首先,利用仿真获得的温度场分布为激光参数调节提供理论依据;其次,通过调节激光功率改变单脉冲能量Ep,结合除锈前后铝合金表面形貌、粗糙度、硬度、残余应力及耐腐蚀性能的变化,对清洗质量进行综合评价,从而确定激光除锈的最优工艺窗口.结果表明,激光除锈效果优于机械打磨,且机械打磨易对铝合金基体造成损伤.在不同激光参数条件下,除锈质量存在显著差异.当0.4 mJ≤Ep≤0.6 mJ时,激光清洗不仅能彻底去除锈蚀,还可提升基体表面的硬度与耐腐蚀性能;Ep过低时,锈蚀残留较多,导致表面粗糙度上升,硬度和耐腐蚀性能下降;Ep过高则容易引起基体表面过烧蚀,损伤材料本体,不利于飞行安全.通过研究得出的参数,不仅能快速有效清除7B04铝合金表面锈蚀,还能维持铝合金表面性能,降低腐蚀对材料造成的终身损害.
The 7B04 aluminum alloy is extensively employed in aerospace structures due to its low density and high specific strength.However,in harsh operational environments,its surface is prone to corrosion,thereby compromising the performance of aerospace systems.To identify a more effective rust removal method and determine the optimal parameters for laser cleaning,a comparative study between laser cleaning and mechanical grinding was conducted through the integration of temperature field simulations and experimental investigations.First,the temperature field distribution derived from simulations provided a theoretical basis for adjusting the laser parameters.Then,by adjusting the laser power to vary the single-pulse energy(Ep),a comprehensive evaluation of cleaning quality was performed based on changes in surface morphology,roughness,hardness,residual stress,and corrosion resistance of the aluminum alloy before and after rust removal.This approach facilitated the identification of the optimal process window for laser cleaning.The results indicated that laser cleaning outperformed mechanical grinding,which is prone to damaging the aluminum substrate.The quality of rust removal varied significantly under varying laser parameter settings.When 0.4 mJ ≤Ep≤ 0.6 mJ,laser cleaning achieved effective corrosion removal and improved the surface hardness and corrosion resistance of the substrate.If Ep was too low,residual rust remained,resulting in increased surface roughness as well as reduced hardness and corrosion resistance.Conversely,if Ep was too high,excessive ablation of the substrate occurred,leading to material degradation that may jeopardize flight safety.The parameters obtained from the study can not only quickly and effectively remove the surface rust of 7B04 aluminum alloy,but also maintain the surface performance of aluminum alloy and reduce the lifelong damage to the material caused by corrosion.
方贵东;宋宇航;单宏斌;沈子实;纪俐
沈阳航空航天大学飞行器快速试制技术研究教育部重点实验室,辽宁沈阳 110136中国人民解放军91331部队,辽宁葫芦岛 125000海装沈阳局,辽宁 沈阳 110032中国飞机强度研究所强度与结构完整性全国重点实验室,陕西西安 710065沈阳航空航天大学飞行器快速试制技术研究教育部重点实验室,辽宁沈阳 110136
航空航天
铝合金激光清洗数值模拟残余应力扫描开尔文探针
aluminium alloylaser cleaningnumerical simulationresidual stressSKP
《航空科学技术》 2026 (7)
75-87,13