新型17Cr4Ni2Mo1Cu三相不锈钢硫化物应力腐蚀开裂行为研究OA

Study on SSC Behavior of Novel 17Cr4Ni2Mo1Cu Triplex Stainless Steel

中文摘要英文摘要

针对油气资源开采向深层、高含H2S苛刻环境发展的需求,研究了新型17Cr4Ni2Mo1Cu三相不锈钢在酸性H2S环境中的应力腐蚀开裂(SSC)行为.利用Thermo-Calc计算相图确定固溶处理工艺,通过EBSD、XRD进行微观表征,并依据NACE TM0177标准A法开展恒载荷SSC试验,结合断口与截面裂纹分析其失效机制.结果表明,试验钢具有高屈服强度(970 MPa),但在苛刻SSC环境下于较短时间内发生脆性断裂;对断口及截面二次裂纹分析表明,裂纹主要沿马氏体区域扩展,而铁素体相表现出优异的耐蚀性;裂纹尖端在扩展过程中遇到铁素体晶粒时会发生偏转,倾向于沿铁素体晶界或寻找马氏体通道继续延伸;马氏体与铁素体之间显著的腐蚀电化学差异是驱动裂纹萌生与早期扩展的关键因素,而铁素体相及其晶界对裂纹尖端扩展路径的阻碍与导向作用,显著影响了SSC裂纹的扩展特征与速率.

The stress corrosion cracking(SSC)behavior of a novel 17Cr4Ni2Mo1Cu triplex stainless steel in acidic H2S enviroment was investigated in response to the demand for deep and high H2S environment in oil and gas extraction.The solution treatment process was determined via phase diagram calculation using Thermo-Calc software.The microstructure of the steel was characterized by X-ray diffraction(XRD)and electron backscatter diffraction(EBSD).SSC tests under constant load were performed in accordance with the NACE TM0177 Standard Method A,and the failure mechanism was analyzed through fracture morphology and cross-sectional crack analysis.The results show that the tested steel exhibits a high yield strength of 970 MPa but it undergoes brittle fracture within a short period of time in a harsh SSC environment.Fracture observation and secondary crack analysis on cross-sections demonstrate that cracks mainly propagate along martensitic regions,while the ferrite phase presents excellent resistance to sulfide stress corrosion.During crack propagation,the crack tip deflects when encountering ferrite grains and tends to extend along ferrite grain boundaries or propagate continuously via martensitic channels.The significant electrochemical corrosion difference between martensite and ferrite phases serves as the core driving factor for crack initiation and early propagation.Moreover,the ferrite phase and its grain boundaries can hinder and guide the propagation of crack tips,which substantially affects the propagation mechanism and growth rate of SSC cracks.

幸雪松;杨芝乐;郑蔚茹;何松;岳小琪;张雷

中海油研究总院有限责任公司,北京 100028||中海石油(中国)有限公司北京研究中心,北京 100028北京科技大学 高精尖学院,北京 100083中海油研究总院有限责任公司,北京 100028||中海石油(中国)有限公司北京研究中心,北京 100028中海油研究总院有限责任公司,北京 100028||中海石油(中国)有限公司北京研究中心,北京 100028北京科技大学 高精尖学院,北京 100083北京科技大学 高精尖学院,北京 100083

矿业与冶金

三相不锈钢硫化氢应力腐蚀开裂微观组织裂纹扩展电化学差异

triplex stainless steelSSCmicrostructurecrack propagationelectrochemical difference

《焊管》 2026 (8)

64-69,6

中国海洋石油有限公司综合科研项目"高温动态腐蚀环境演化与经济型油套管防腐技术研究"(项目编号KJZH-2024-2301).

10.19291/j.cnki.1001-3938.2026.08.007

评论