交流干扰下缺陷尺寸对涂层剥离区X80钢腐蚀行为的影响OA
Effect of Defect Size on X80 Steel Corrosion Behavior in Coating Delamination Zone under AC Interference
针对交流杂散电流与防腐涂层破损协同作用引发的埋地管线失效问题,以X80钢为研究对象,研究了不同涂层缺陷尺寸(0 mm、0.2 mm、1 mm)对剥离涂层下X80钢腐蚀行为的影响.结果表明,交流干扰诱导的界面碱化显著加速了涂层剥离过程,缺陷尺寸决定了局部腐蚀的演化走向,0.2 mm微小缺陷由于被铁氧化物覆盖,使得该处的阻抗升高,由于形成酸化闭塞电池,使缺陷处局部腐蚀加剧;而当缺陷增大至1 mm时,腐蚀产物失去屏障保护作用,缺陷处发生横向剥蚀.有限元分析结果表明,剥离涂层缺陷越小,瞬时电流在中心区域的"八芒星"状聚集效应越明显,从而表明微小缺陷在交流场下具有更高的点蚀穿孔风险.研究结果可为交流干扰下埋地管线的安全评估与防护提供理论支撑.
To address the issue of buried pipeline failure caused by the synergistic effect of AC stray currents and damage to anti-corrosion coatings,it takes X80 steel as the research object,and investigates the influence of different initial defect sizes(0 mm,0.2 mm and 1 mm)on the corrosion behaviour of the delaminated coating X80 steel system.The results show that AC-induced interfacial alkali contamination significantly accelerated the coating delamination process;the size of the defect determines the progression of localized corrosion.At a minute defect of 0.2 mm,the presence of iron oxide plugging causes the increasing of the impedance at this location.However,the formation of an acidfield occlusion battery exacerbates localized corrosion at the defect site.When the defect enlarges to 1 mm,the corrosion products lose their protective barrier function,resulting in lateral corrosion at the defect site.Finite element analysis further revealed that the smaller the defect in the delaminated coating,the more pronounced the eight-pointed star pattern of instantaneous current concentration in the central region,implying that microdefects present a higher risk of pitting and perforation under alternating current conditions.The research results can provide theoretical support for the safety assessment and protection of buried pipelines under alternatingcurrent interference.
万红霞;刘义;刘茹;宋冬冬
中国石油大学(北京)新能源与材料学院,北京 102249中国石油大学(北京)新能源与材料学院,北京 102249中国石油大学(北京)新能源与材料学院,北京 102249华北电力大学 电站能量传递转化与系统教育部重点实验室,北京 102206
矿业与冶金
X80管线钢杂散电流腐蚀涂层缺陷尺寸有限元仿真
X80 pipeline steelstraycurrent corrosioncoating defect sizefiniteelement simulation
《焊管》 2026 (8)
22-32,11