首页|期刊导航|焊管|X80钢在典型土壤环境中的腐蚀及SCC行为机理研究

X80钢在典型土壤环境中的腐蚀及SCC行为机理研究OA

Mechanistic Study on Corrosion and SCC Behavior of X80 Steel in Typical Soil Environments

中文摘要英文摘要

针对埋地管道因腐蚀引发泄漏失效等问题,以我国南方酸性土壤(鹰潭)和西北高盐碱性土壤(哈密)两种典型环境为例,通过均匀腐蚀试验、电化学试验、慢应变速率拉伸(SSRT)试验、腐蚀特征微观表征等方法,系统研究了X80钢两种环境下的腐蚀行为.结果显示,X80钢在两种模拟溶液无应力条件下均匀腐蚀行为比较一致,均表现为均匀腐蚀为主,并伴有点蚀发生,腐蚀速率等级接近,均随浸泡时间延长呈负指数幂函数关系衰减;在应力加载条件下,X80钢在两种环境不同影响因素下的SCC敏感性总体偏低.两种介质中阴极电位对其SCC行为的影响趋势基本一致,从开路电位(OCP)至-850 mV的电位,SCC敏感性略有升高;从-850 mV至-1 200 mV电位,SCC敏感性快速增大,其在哈密土壤模拟溶液中的SCC敏感性总体高于鹰潭土壤模拟溶液.综合分析表明,合理阴极保护电位能够兼顾X80钢的均匀腐蚀和SCC防护.

To address issues such as leakage and failure caused by corrosion in buried pipelines,the corrosion behavior of X80 steel in two typical environments:acidic soil in southern China(Yingtian)and highly saline-alkali soil in northwestern China(Hamit)is systematically investigated.Methods included uniform corrosion tests,electrochemical tests,slow strain rate tensile(SSRT)tests,and microscopic characterization of corrosion features.The results indicate that X80 steel presents consistent uniform corrosion behavior in the two simulated solutions under stress-free conditions,with a corrosion mode dominated by uniform corrosion accompanied by pitting corrosion.The corrosion rates in the two solutions are at similar levels,and both decay following a negative exponential power function with the extension of immersion time.Under stressed conditions,X80 steel exhibits generally low SCC susceptibility under different influencing factors in the two soil environments.Cathodic potential exerts a similar effect on the SCC behavior of X80 steel in both solutions.The SCC susceptibility increases slightly when the potential changes from the open circuit potential(OCP)to-850 mV,and rises sharply as the potential decreases from-850 mV to-1 200 mV.Overall,the SCC susceptibility of X80 steel in the Hami soil simulated solution is higher than that in the Yingtan soil simulated solution.Comprehensive analysis shows that the conventional cathodic protection potential can realize dual protection against uniform corrosion and stress corrosion cracking for X80 steel.

闫立震;张丽丽;代文贺;刘智勇

北京科技大学 新材料技术研究院,北京 100083北京科技大学 新材料技术研究院,北京 100083河北省特种设备监督检验研究院,石家庄 050061||国家市场监督管理总局重点实验室(钢制管子及管件安全评价),石家庄 050061北京科技大学 新材料技术研究院,北京 100083||国家市场监督管理总局重点实验室(钢制管子及管件安全评价),石家庄 050061

矿业与冶金

X80钢土壤腐蚀均匀腐蚀应力腐蚀开裂腐蚀机理

X80 steelsoil corrosionuniform corrosionstress corrosion crackingcorrosion mechanism

《焊管》 2026 (8)

13-21,32,10

国家市场监督管理总局科技计划项目"高强钢制管道应力腐蚀开裂在线评价方法与测试装置研究"(项目编号2024MK011).

10.19291/j.cnki.1001-3938.2026.08.002