改性聚苯醚发泡珠粒的制备及其性能研究OA
Preparation and properties of modified polyphenylene ether foam beads
以聚苯醚(PPE)为基体、高抗冲聚苯乙烯(HIPS)为加工改性剂,通过引入聚对苯二甲酸乙二醇酯(PET)或聚酰胺6(PA6)作为分散相组分,并配以磷系阻燃剂RDP/BDP及SEBS-g-MAH、环氧扩链剂增容扩链体系,制备了阻燃改性聚苯醚(MPPE)微粒;以超临界CO2为发泡剂经釜压发泡制备MPPE发泡珠粒,并通过蒸汽模塑成型获得MPPE发泡珠粒制品.结果表明,PPE/HIPS/PET为55/30/15注塑样品的拉伸强度为67.7 MPa、悬臂梁缺口冲击强度为21.0 kJ/m2、阻燃达UL 94 V-0级,其发泡珠粒平均泡孔直径仅2.74 μm、泡孔密度达1.71×1010 个/cm3、表观密度低至0.095 g/cm3.制品密度由99 kg/m3增至297 kg/m3时,压缩强度由0.70 MPa增至4.51 MPa,拉伸强度由0.59 MPa增至3.36 MPa,导热系数由0.040 W/(m·K)增至0.058 W/(m·K),低密度制品兼具良好的力学性能与优异的隔热性能.
Modified polyphenylene ether(MPPE)foam beads were prepared via supercritical CO2 bead foaming.Poly-phenylene ether(PPE)was blended with high-impact polystyrene(HIPS),and polyethylene terephthalate(PET)or polyamide 6(PA6)was introduced as the dispersed phase,with RDP/BDP as flame retardants and SEBS-g-MAH/ep-oxy chain extender as the compatibilization and chain-extension system.The MPPE microbeads were foamed in an auto-clave with supercritical CO2 and then molded by steam chest molding.The results show that the injection-molded speci-mens of the optimal formulation(PPE/HIPS/PET=55/30/15)exhibited a tensile strength of 67.7 MPa,a notched Izod impact strength of 21.0 kJ/m2 and a UL 94 V-0 rating,and the corresponding foam beads possessed an average cell diameter of 2.74 μm,a cell density of 1.71×1010 cells/cm3 and an apparent density of 0.095 g/cm3.As the product den-sity increased from 99 kg/m3 to 297 kg/m3,the compressive strength increased from 0.70 MPa to 4.51 MPa,the tensile strength from 0.59 MPa to 3.36 MPa,and the thermal conductivity increased from 0.040 W/(m·K)to 0.058 W/(m·K).The low-density products combine good mechanical properties with excellent thermal insulation performance.
刘亦枫;卢泰晨;刘本刚
四川大学匹兹堡学院,成都 610207河北明润复合材料科技有限公司,河北 衡水 053700河北明润复合材料科技有限公司,河北 衡水 053700||北京阜泉科技有限公司,北京 101105
化学化工
改性聚苯醚发泡珠粒异相成核泡孔结构超临界二氧化碳
modified polyphenylene etherfoam beadsheterogeneous nucleationcellular structuresupercritical carbon dioxide
《中国塑料》 2026 (8)
56-62,7
评论