首页|期刊导航|中国造纸|基于TG-FTIR和原位红外法的油斑卷烟纸热解特性及产物分析

基于TG-FTIR和原位红外法的油斑卷烟纸热解特性及产物分析OA

Analysis on the Pyrolysis Characteristic and Products of Oil-spotted Cigarette Paper Using TG-FTIR and In Situ Infrared Spectroscopy

中文摘要英文摘要

本研究通过热重红外联用仪(TG-FTIR)、程序控温加热平台耦连热解产物捕集分析,以及原位傅里叶变换红外光谱仪(in situ FT-IR)结合二维相关红外光谱(2D-COS)分析等手段,探究了润滑油污染物对卷烟纸表面化学结构、热解过程、热解气固相产物特征及热解路径的影响.结果表明,润滑油污染物可浸染卷烟纸表面纤维,表面官能团呈现明显的长碳链烷烃类物质吸收峰,润滑油组分与卷烟纸填料间存在相互作用.油斑卷烟纸的纤维素分解阶段(热解阶段Ⅱ)最大质量损失速率降至12.12%/min,热解阶段Ⅱ的最大质量损失速率温度、炭化成焦阶段(热解阶段Ⅲ)的质量损失率及终止热解温度均升高,且综合热解指数降至2.07×10-4%/(min·℃²),热解阶段Ⅲ的反应动力学机理改变且活化能降低.油斑卷烟纸热解产物的复杂度增加,高温热解条件下的烃类、酯类等热解产物相对含量升高,稠环芳烃类物质检出,2D-COS分析表明,表面润滑油污染改变了卷烟纸热解反应路径.

This study employed thermogravimetry-fourier transform infrared spectroscopy(TG-FTIR),a programmable heating platform cou-pled with a pyrolysis product collection system,and in situ fourier transform infrared spectroscopy(in situ FT-IR)combined with two-dimen-sional correlation spectroscopy(2D-COS),to investigate the effects of lubricating oil contaminants on the surface chemistry structure,pyroly-sis process,gaseous and solid pyrolysis products,and pyrolysis pathways of cigarette paper.The results showed that lubricating oil contami-nants infiltrated the fiber on the surface of cigarette paper,and the surface functional groups exhibited distinct long-chain alkane substances absorption peaks,indicating interactions between the lubricating oil components and the fillers in the cigarette paper.For oil-stained ciga-rette paper,the maximum mass loss rate during the cellulose decomposition stage(pyrolysis stage Ⅱ)decreased to 12.12%/min;the peak temperature of pyrolysis stage Ⅱ,the mass loss percentage and the final pyrolysis temperature of charring stage(pyrolysis stage Ⅲ)all in-creased;the comprehensive pyrolysis index decreased to 2.07×10-4%/(min·℃2),and the reaction kinetic mechanism of the pyrolysis stageⅢ changed,accompanied by a decrease in activation energy.There was increased complexity of pyrolysis products from oil-stained ciga-rette paper.Under high-temperature pyrolysis conditions,the relative contents of hydrocarbons,esters,and other species increased,and polycyclic aromatic hydrocarbons were detected.The 2D-COS analysis showed that lubricating oil contamination on the cigarette paper sur-face altered the pyrolysis reaction pathway.

崔升;向科宇;刘于干;黄江;赫林林;康金岭;张峻松;梁淼;刘大卫

广西中烟工业有限责任公司,广西 南宁,530001郑州轻工业大学烟草科学与工程学院,河南 郑州,450000广西中烟工业有限责任公司,广西 南宁,530001广西中烟工业有限责任公司,广西 南宁,530001广西中烟工业有限责任公司,广西 南宁,530001广西中烟工业有限责任公司,广西 南宁,530001郑州轻工业大学烟草科学与工程学院,河南 郑州,450000郑州轻工业大学烟草科学与工程学院,河南 郑州,450000广西中烟工业有限责任公司,广西 南宁,530001

轻工纺织

油斑卷烟纸热重红外原位红外热解

oil-stained cigarette paperTG-FTIRin situ FT-IRpyrolysis

《中国造纸》 2026 (8)

197-207,11

广西中烟工业有限责任公司科技项目(GXZY-CX2023A002).

10.11980/j.issn.0254-508X.2026.08.021

评论