荧光增白剂ER-Ⅰ的分散稳定性影响因素OA
Influencing factors of dispersion stability of fluorescent whitening agent ER-Ⅰ
为提高涤纶用液体荧光增白剂的分散稳定性,以增白剂ER-I为例,本研究采用单因素分析法和正交实验法考察颗粒粒径、分散剂种类、增白剂与分散剂质量比以及增白剂用量等因素对分散体系稳定性的影响.结果表明,各因素影响程度从大到小为:颗粒粒径、分散剂种类、增白剂与分散剂质量比、增白剂用量.当使用超分散剂、在增白剂用量为1 g/L、增白剂与分散剂质量比为1.0∶0.5,增白剂平均粒径为200 nm水平时,可获得最佳稳定效果,离心残留率达到59.5%,静置稳定性也得到显著提升.同时,优化体系对涤纶织物具有良好的增白效果.
To improve the dispersion stability of liquid fluorescent whitening agents for polyester,taking whitening agent ER-I as an example,this study used single factor analysis and orthogonal experimental meth-ods to investigate the effects of particle size,dispersant type,mass ratio of whitening agent to dispersant,and whitening agent dosage on the stability of the dispersion system.The results indicate that the degree of influence of each factor,from large to small,is as follows:particle size,type of dispersant,mass ratio of whit-ening agent to dispersant,and dosage of whitening agent.When using a super dispersant,the concentration of the whitening agent is 1 g/L,the mass ratio of the whitening agent to the dispersant is 1.0∶0.5,and the av-erage particle size of whitening agent is around 200 nm,the best stability effect is obtained,with a residual concentration of 59.5%after centrifugation.The static stability has also been significantly improved.Mean-while,the optimized system has a good whitening effect on polyester fabrics.
张博;季正芳;江华
浙江理工大学生态染整技术教育部工程研究中心,浙江 杭州 310018浙江弘毅化学有限公司,浙江 丽水 323700||浙江道远新材料有限公司,浙江 丽水 322700||浙江法斯特新材料有限公司,浙江 丽水 322700浙江理工大学生态染整技术教育部工程研究中心,浙江 杭州 310018||浙江道远新材料有限公司,浙江 丽水 322700
化学化工
荧光增白剂稳定性超分散剂白度
fluorescent whitening agentstabilitysuper dispersantwhiteness
《印染助剂》 2026 (8)
23-27,5