高速铁路CRTSⅢ型板自密实混凝土离缝成因与防治研究OA
Study on the causes and prevention of open jointing in self-compacting concrete of CRTSⅢ type slab track for high-speed railway
文章针对无砟轨道 CRTSⅢ型板自密实混凝土填充层与轨道板之间出现的离缝问题,基于系统实验和现场实践,多方面系统分析离缝成因.首先从材料性能角度出发,分析了自密实混凝土的收缩特性、配合比设计以及早期强度发展对界面黏结性能的影响;从施工工艺角度,研究了浇筑方式、环境温湿度控制以及扣件压力对混凝土均匀性和密实性的作用;结合结构受力和变形协调机制,讨论了轨道板与混凝土层之间的变形差异及其引发的应力集中现象.在此基础上,进一步提出了针对性的裂缝预防措施,包括优化混凝土材料配比、加强施工过程控制、完善养护制度等.文章为提升自密实混凝土施工质量、减少离缝发生提供理论依据与实践指导.
To address the issue of interfacial gaps(debonding)between the self-compacting concrete(SCC)fill-ing layer andtrack slab in the CRTS Ⅲ ballastless track system,this paper systematically analyzes the causes of such defects through laboratory tests and field practices.First,from the perspective of material properties,the study investigates the influence of shrinkage characteristics,mix proportion design,and early-age strength gain of the SCC on interfacial bonding performance.Second,regarding construction techniques,the effects of casting methods,ambient temperature and humidity control,and fastener clamping pressure on the uniformity and compactness of the concrete are examined.Furthermore,incorporating the mechanisms of structural loading and deformation compatibility,the paper discusses the differential deformation between the track slab and the concrete layer,as well as the concentration stress phenomena.Based on these analyses,targeted preventive countermeasures are proposed,including the optimization of concrete mix proportions,the reinforcement of construction process control,and the improvement of curing regimes.This research provides a theoretical basis and practical guidance for enhancing the construction quality of self-compacting concrete and mitigating the oc-currence of interfacial gaps.
杨明志;张卫红;杨锦涛
中国水利水电第五工程局有限公司,四川 成都 610207中国水利水电第五工程局有限公司,四川 成都 610207中国水利水电第五工程局有限公司,四川 成都 610207
交通工程
无砟轨道CRTSⅢ型板自密实混凝土离缝
CRTS Ⅲ slab ballastless trackself-compacting concrete(SCC)debonding
《四川水力发电》 2026 (z1)
146-150,5
评论