干热环境户外自然老化对钢结构防火涂层性能的影响OA
Effect of Outdoor Natural Dry-hot Environment Aging on the Performances of Fire-retardant Coating for Steel Structure
选择新疆典型干热气候地区对涂覆防火涂层的钢结构试样进行自然老化试验,研究了防火涂层的不同结构和老化时间对其外观形貌、粘结强度、耐火性能的影响.结果表明,随着老化时间的增加,FC-PIT涂层的表面洁净度、粘结强度和耐火性能下降,经自然老化6个月后,FC-PIT涂层仍能保持良好的完整性、钢表面附着力和耐火性能,而未使用底漆、中间漆或面漆的FC-IT、FC-PT、FC-PI涂层出现不同程度的破损,并丧失粘附性和防火能力.与未老化FC-PIT相比,老化6个月FC-PIT涂层的粘结强度、耐火极限、膨胀倍率分别为1.33 MPa、48 min、28,分别衰减了 20.8%、9.4%、9.8%,保持了良好的钢基材表面附着力和耐火性能.该研究为干热环境下防火涂层的老化机制和工程应用提供指导.
Outdoor natural aging experiment in a typical dry-hot environment was carried out to investigate the effects of the structure and aging time of the fire-retardant coatings for steel structure samples on their apparent morphology,adhesion strength and fire resistance.The results showed that the surface cleanliness,adhesion strength and fire resistance of the FC-PIT coatings deteriorated with the increase of aging time.After six months of natural aging,the FC-PIT can still maintain good integrity,steel surface adhesion and fire resistance.Whereas the FC-IT,FC-PT and FC-PI coatings without primer,intermediate or topcoat layer exhibit varying degrees of damage,resulting in the loss of surface adhesion and fire resistance on steel structure.In comparison with the unaged FC-PIT,the adhesion strength,fire resistance limit and expansion ratio of the FC-PIT coating after ageing 6 months were 1.33 MPa,48 min and 28,respectively.The corresponding attenuation rates for adhesion strength,fire resistance limit and expansion ratio of the aged FC-PIT sample were 20.8%,9.4%and 9.8%,respectively,retaining strong adhesion to the steel substrate and effective fire resistance.This work provides guidance for the aging mechanism and engineering application of fire-retardant coatings in dry-hot environments.
唐全宏;张天昊;魏捷;梅晶;黄建敏;侯春生;王敏臣
中国石油天然气集团有限公司超深层复杂油气藏勘探开发技术研发中心,新疆库尔勒 841000||新疆维吾尔自治区超深层复杂油气藏勘探开发工程研究中心,新疆库尔勒 841000||新疆超深油气重点实验室,新疆库尔勒 841000||塔里木油田公司,新疆库尔勒 841000应急管理部四川消防研究所,四川成都 610036中国石油天然气集团有限公司超深层复杂油气藏勘探开发技术研发中心,新疆库尔勒 841000||新疆维吾尔自治区超深层复杂油气藏勘探开发工程研究中心,新疆库尔勒 841000||新疆超深油气重点实验室,新疆库尔勒 841000||塔里木油田公司,新疆库尔勒 841000新疆维吾尔自治区应急管理科学研究院,新疆乌鲁木齐 830000中国石油天然气集团有限公司超深层复杂油气藏勘探开发技术研发中心,新疆库尔勒 841000||新疆维吾尔自治区超深层复杂油气藏勘探开发工程研究中心,新疆库尔勒 841000||新疆超深油气重点实验室,新疆库尔勒 841000||塔里木油田公司,新疆库尔勒 841000中国石油天然气集团有限公司超深层复杂油气藏勘探开发技术研发中心,新疆库尔勒 841000||新疆维吾尔自治区超深层复杂油气藏勘探开发工程研究中心,新疆库尔勒 841000||新疆超深油气重点实验室,新疆库尔勒 841000||塔里木油田公司,新疆库尔勒 841000新疆维吾尔自治区应急管理科学研究院,新疆乌鲁木齐 830000
化学化工
钢结构防火涂层涂层结构自然老化干热环境耐火性能
fire-retardant coatings for steel structurecoating structurenatural agingdry-hot environmentfire resistance
《合成材料老化与应用》 2026 (4)
5-9,5