超超临界机组S30432受热面失效机理研究OA
Research on the Failure Mechanism of S30432 Heating Surface in Ultra Supercritical Unit
通过对不同服役周期的S30432过热爆管进行显微组织分析、扫描电镜和能谱分析、透射电镜分析、室温拉伸试验、室温冲击试验和高温拉伸试验,研究了 S30432受热面失效机理.结果表明:S30432过热爆管失效均符合蠕变开裂的特征,晶界处析出长大的块状M23C6相或σ相,促进了蠕变裂纹的形成;不同服役周期下,爆管组织中晶界析出相种类不同,短周期过热主要析出M23C6相,随服役周期延长部分M23C6相转化为有害σ相;S30432受热面金属监督中应重点检查塑韧性和高温强度等性能劣化情况,以降低由此引发早期失效的风险.
The failure mechanism of S30432 heating surface was studied by conducting microstructure analysis,scanning electron microscopy and energy spectrum analysis,transmission electron microscopy analysis,room temperature tensile test,room temperature impact test,and high temperature tensile test on S30432 cracked tubes after different service cycles.The results show that failure mode of S30432 overheated tubes all conform to the characteristics of creep cracking,and the precipitation of large block M23C6 phase or σ phase at the grain boundary promotes the formation of creep cracks.Under different service cycles,the types of crystal boundary precipitates in the explosive tubes are different,short cycle overheating mainly precipitates M23 C6 phase,while some M23 C6 phase transforms into harmful σ phase with the extension of service cycle.In the supervision of S30432 heating surface,the focus should be on checking the deterioration of properties such as plasticity,toughness,and high-temperature strength,to reduce the risk of early failure caused by this.
杨希锐;李世涛;李艳军;邓雷凯;张宁;高立行;马东方;胡锋涛
润电能源科学技术有限公司,河南郑州 450000润电能源科学技术有限公司,河南郑州 450000润电能源科学技术有限公司,河南郑州 450000华润电力湖北有限公司,湖北咸宁 437000深圳市深汕特别合作区华润电力有限公司,广东 深圳 518230华润电力菏泽有限公司,山东菏泽 274000润电能源科学技术有限公司,河南郑州 450000润电能源科学技术有限公司,河南郑州 450000
能源科技
S30432过热失效机理晶界析出相蠕变失效
S30432overheatingfailure mechanismgrain boundary precipitation phasecreep failure
《锅炉技术》 2026 (4)
46-51,6
华润电力控股有限公司重大科技研发项目(CRP-R&D-LX-2024-004)
评论