电厂锅炉高温再热管烟气侧高温腐蚀原因分析OA
Analysis on Corrosion on Flue Gas Side of High Temperature Reheater Tubes in Power Plant Boiler
针对某电厂高温再热器烟气侧高温腐蚀严重问题,通过宏观分析、微观观察、扫描电镜和能谱成分测试以及常温力学测试,分析了某电厂使用约4万h的TP347HFG锅炉高温再热器管的高温腐蚀原因.结果表明:管材老化程度为3级;受壁温差异影响,迎烟面硬度、抗拉强度、屈服强度均低于背烟面,但塑性较好,整体力学性能仍符合ASTM A213/A213M-2019标准.锅炉配风不均和局部烟气中高浓度的SO2、CO是造成高温腐蚀的主要原因,主要表现为硫腐蚀和还原气氛引起的腐蚀.
In view of the serious problem of high-temperature corrosion on the flue gas side of the high-temperature reheater of a power plant,the causes of high-temperature corrosion of the high-temperature reheater tube of a TP347HFG boiler used for about 40,000 hours in a power plant were analyzed through macroscopic analysis,microscopic observation,scanning electron microscopy,energy spectrum composition test and room temperature mechanical test.The results showed that the aging degree of the reheater tubes reached grade 3.Due to the temperature difference between the flue gas side and rear side,the hardness,tensile strength and yield strength of the flue gas side are lower than those of the rear side,but the elongation is higher.The mechanical properties of both meet the ASTM A213/A213M-2019 standard.The high concentration of SO2 and CO in the uneven boiler air supply and local flue gas is the main cause of high-temperature corrosion,which is mainly manifested as sulfur corrosion and corrosion caused by reducing atmosphere.
罗昌福;胡明;李文博;地里扎提·地里夏提;杨博闻;祁博武;李鹏辉
华电电力科学研究院有限公司,浙江 杭州 310030华电电力科学研究院有限公司,浙江 杭州 310030华电电力科学研究院有限公司,浙江 杭州 310030华电电力科学研究院有限公司,浙江 杭州 310030华电电力科学研究院有限公司,浙江 杭州 310030华电电力科学研究院有限公司,浙江 杭州 310030华电电力科学研究院有限公司,浙江 杭州 310030
矿业与冶金
TP347HFG常温力学性能高温腐蚀
TP347HFGroom temperature mechanical propertieshigh-temperature cor-rosion
《锅炉技术》 2026 (4)
41-45,5