首页|期刊导航|福建冶金|Φ100~Φ160 mm规格圆钢轧制工艺表面裂纹形成机理与控制策略

Φ100~Φ160 mm规格圆钢轧制工艺表面裂纹形成机理与控制策略OA

Formation Mechanism and Control Strategy of Surface Cracks in Φ100~Φ160 mm Round Steel Rolling Process

中文摘要英文摘要

针对中大规格圆钢高速轧制时表面裂纹频发、尤其角部浅表裂纹占比高的问题,研究孔型结构与轧制节奏对裂纹的耦合影响.通过缺陷分析、金相检测与工艺追溯,确定连铸残余、孔型支撑不足及温差应力梯度为裂纹主因.热力耦合仿真表明,开坯第 5~7 道次为裂纹高发区,沿角部应力集中路径扩展.据此提出侧壁斜度调整、槽口优化与轧速分区控制的联动策略.试轧验证该方案显著降低裂纹率,提升表面质量与成品一致性,为工艺优化提供理论依据.

Addressing the frequent occurrence of surface cracks,particularly the high proportion of shallow corner cracks in medium-to-large round steel during high-speed rolling,this study investigates the coupled effects of pass geometry and rolling rhythm on crack formation.Through defect analysis,metallographic examination,and process tracing,continuous casting residuals,insufficient pass support,and thermal stress gradients are identified as the main causes of cracking.Thermo-mechanical coupling simulations indicate that the 5th to 7th roughing passes are high-risk zones for cracking,with cracks propagating along corner stress concentration paths.Accordingly,an integrated strategy involving sidewall taper adjustment,groove optimization,and zone-based rolling speed control is proposed.Pilot rolling trials demonstrate that this scheme significantly reduces the crack incidence and improves surface quality and product consistency,providing a theoretical basis for process optimization.

郑欣炫

三钢闽光股份有限公司,福建 三明 353000

Φ100~Φ160 mm规格圆钢表面裂纹孔型结构轧制节奏热力耦合仿真

Φ100~Φ160 mm round steelsurface crackspass geometryrolling rhythmthermo-mechanical coupling simulation

《福建冶金》 2026 (5)

33-35,3

评论