Effects of Welding Thermal Cycle and Post-Weld Aging on the Micro-structure and Mechanical Properties of GH2070P Fe-Ni-Based Superalloy Welded Joints

中文摘要英文摘要

针对新型铁镍基高温合金GH2070P在时效状态下进行钨极氩弧焊(GTAW),研究焊接热循环及焊后时效处理对焊接接头显微组织与室温力学性能的影响规律.焊接接头两侧母材分别经800℃/20 h和800℃/4 h焊前预热处理,焊后进行800℃/4 h时效处理.结果表明,焊态接头宏观及微观组织完好,母材及热影响区主要析出相为MC、M23C6和γ'相,焊缝主要析出相为M6C、MC及少量γ'相,未见其他有害析出相.焊接热循环导致HAZ中M23C6部分回溶、γ'相大量回溶,硬度大幅降低、存在1.5 mm宽的软化区,室温拉伸试样于HAZ断裂;经800℃/4 h时效强化热处理后,HAZ晶界M23C6及晶内γ'相重新弥散析出,焊缝基体亦析出少量γ'相,软化区硬度恢复至母材水平,拉伸断裂位置由HAZ转移至焊缝中心,接头抗拉强度与屈服强度分别提升23.3%和16.1%.研究证实,焊后时效处理可有效消除GH2070P焊接接头HAZ软化问题,为该合金在650℃及以上超超临界锅炉中的焊接应用提供了试验依据.

The gas tungsten arc welding(GTAW)of the precipitation-strengthened Fe-Ni-based superalloy GH2070P in the aged condition was investigated,with emphasis on the influence of welding thermal cycling and post-weld heat treatment(PWHT)on the microstructural evolution and room-temperature mechanical properties of the welded joints.The base metals on each side of the joint were pre-treated at 800℃for 20 h and 4 h,respectively,followed by post-weld aging at 800℃for 4 h.The results reveal that the as-welded joint is free of macroscopic and microscopic defects.The precipitates in the base metal(BM)and heat-affected zone(HAZ)are identified as MC,M23C6,and γ' phases,while the weld metal(WM)contains M6C,MC,and a trace amount of γ'.The welding thermal cycle causes partial dissolution of M23C6 carbides and substantial dissolution of γ' precipitates in the HAZ,producing a softened zone approximately 1.5 mm in width,where tensile fracture occurs at room temperature.Following PWHT at 800℃for 4 h,M23C6 carbides and γ' precipitates re-precipitate in a fine,dispersed distribution within the HAZ,and a small quantity of γ' phase also forms in the WM.The hardness of the softened zone recovers to the BM level,and the tensile fracture location shifts from the HAZ to the WM center,with the tensile strength and yield strength increasing by 23.3%and 16.1%,respectively.The study demonstrates that post-weld aging effec-tively eliminates the HAZ softening problem in GH2070P welded joints,providing experimental support for the welding ap-plication of this alloy in ultra-supercritical boilers operating at 650℃and above.

张松;徐祥久;刘海;刁旺战;王萍;赵卫君

哈尔滨锅炉厂有限责任公司,黑龙江 哈尔滨 150046||低碳热力发电技术与装备全国重点实验室,黑龙江 哈尔滨 150046哈尔滨锅炉厂有限责任公司,黑龙江 哈尔滨 150046||低碳热力发电技术与装备全国重点实验室,黑龙江 哈尔滨 150046哈尔滨锅炉厂有限责任公司,黑龙江 哈尔滨 150046||低碳热力发电技术与装备全国重点实验室,黑龙江 哈尔滨 150046哈尔滨锅炉厂有限责任公司,黑龙江 哈尔滨 150046||低碳热力发电技术与装备全国重点实验室,黑龙江 哈尔滨 150046哈尔滨锅炉厂有限责任公司,黑龙江 哈尔滨 150046||低碳热力发电技术与装备全国重点实验室,黑龙江 哈尔滨 150046哈尔滨锅炉厂有限责任公司,黑龙江 哈尔滨 150046||低碳热力发电技术与装备全国重点实验室,黑龙江 哈尔滨 150046

矿业与冶金

GH2070P高温合金钨极氩弧焊ERNiCrCoMo-1焊接热循环析出相与软化行为

GH2070P superalloygas tungsten arc welding(GTAW)ERNiCrCoMo-1welding thermal cycleprecipitate dissolution and softening behavior

《电焊机》 2026 (8)

97-104,8

国家重点研发计划(2023YFB4102303)

10.7512/j.issn.1001-2303.2026.08.10

评论