中文摘要英文摘要

针对Haynes 230/Inconel 617异种高温合金精密连接及高温服役需求,采用BNi2非晶镍基钎料开展真空钎焊试验,固定保温时长15 min,设置1 015℃、1 035℃两组钎焊温度.通过润湿试验、室温剪切及750℃高温剪切试验,系统探究钎焊温度对钎料润湿铺展性能、异种接头常温及高温力学性能的影响规律.结果表明:钎焊温度提升对钎料润湿性能存在母材差异化影响,升温可大幅提高BNi2钎料在Haynes 230合金表面的铺展面积(平均润湿面积提升132.9%),但对Inconel617表面润湿性能无明显改变;低温工艺(1 015℃/15 min)接头室温剪切性能与高温力学稳定性俱佳,室温平均剪切强度达206.96 MPa,750℃高温平均剪切强度为126.88 MPa;高温工艺(1 035℃/15 min)钎料铺展均匀性更优,但界面扩散层较宽易生成脆性相,导致接头高温力学性能下降.基于试验数据揭示了钎焊温度—润湿行为—力学性能的关联机制,可为镍基异种高温合金钎焊工艺优化及工程应用提供数据支撑.

To meet the requirements of precision joining and high-temperature service of dissimilar Haynes 230 and Inconel 617 superalloys,vacuum brazing experiments were carried out using amorphous nickel-based BNi2 filler metal.With the holding time fixed at 15 min,two brazing temperatures of 1 015℃and 1 035℃were designed.Wetting tests,room-temperature shear tests and high-temperature shear tests at 750℃were performed to systematically investigate the effects of brazing temperature on the wetting and spreading characteristics of the filler metal,as well as the room-temperature and high-temperature mechanical properties of the dissimilar joints.The results reveal that increasing brazing temperature exerts differentiated influences on the filler wetting behavior for the two base metals.Temperature rise significantly improves the spreading performance of BNi2 filler on Haynes 230 substrate,while it imposes no obvious variation on the wetting property over Inconel 617.The joint fabricated at the low-temperature process(1 015℃/15 min)exhibits excellent room-temperature shear strength and superior high-temperature mechanical stability,with an average room-temperature shear strength of 206.96 MPa and an average high-temperature shear strength of 126.88 MPa at 750℃.Although the high-temperature pro-cess(1 035℃/15 min)achieves more uniform spreading of the filler metal,the excessively thick interfacial diffusion layer facilitates the formation of brittle phases,thereby deteriorating the high-temperature mechanical properties of the joint.The correlation mechanism among brazing temperature,wetting behavior and mechanical properties is clarified based on experi-mental data.This work can provide reliable data support for process optimization and engineering application of vacuum brazing of dissimilar nickel-based superalloy joints.

刘德运;郭瑞臻;李云月;畅海丞;赵凯;秦建

中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001北京星航机电装备有限公司,北京 100074中国机械总院集团郑州机械研究所有限公司 高性能新型焊接材料全国重点实验室,河南 郑州 450001

矿业与冶金

BNi2非晶钎料Haynes230合金Inconel617合金真空钎焊润湿性能力学性能

BNi2Haynes 230 alloyInconel 617 alloyvacuum brazingwettabilitymechanical properties