首页|期刊导航|采矿与岩层控制工程学报|弱胶结充填体强度特性及其对重金属浸出抑制机理

弱胶结充填体强度特性及其对重金属浸出抑制机理OA

Strength characteristics of weakly cemented backfill and its inhibition mechanism on heavy metal leaching

中文摘要英文摘要

胶结充填体的强度设计需同时保障采场稳定与控制重金属浸出风险,然而长期服役环境下其强度劣化机理与胶材掺量临界条件仍不明确.因此,针对 Pb、Cu、Zn、Cr 四种重金属,通过静态浸出、SEM 与 XRD试验,研究了弱胶结充填体在化学侵蚀下的性能演化规律.研究结果表明:①重金属 Cr稳定性最高,Pb 和 Zn 次之,而 Cu 最易受环境和化学性质影响发生形态演化.②充填体长期稳定性高度依赖于环境 pH值,pH=7 条件下 1∶10 配比试样 90 d 强度最高(2.11 MPa),pH=10条件下 1∶20 配比试样 90 d 强度最低(0.63 MPa),酸性条件引发早期侵蚀,碱性环境导致后期膨胀劣化.③灰砂比对重金属固化效果影响显著.1∶20 配比下 Pb、Cu、Zn、Cr的浸出含量最高,分别为 0.000 95、0.94、0.86、0.014 7 mg/L,是 1∶10 配比的 2~3 倍,均符合《地下水质量标准》(GB/T 14848-2017)Ⅲ类标准.研究结果明确了环境-配比-性能间的关联,可为绿色矿山充填设计提供参考.

The strength design of cemented backfill must simultaneously ensure stope stability and control the risk of heavy metal leaching.However,the mechanisms of long-term strength degradation and the critical condition for binder dosage remain unclear under prolonged service environments.Accordingly,this study investigates the performance evolution of weakly cemented backfill under chemical erosion,targeting four heavy metals(Pb,Cu,Zn,Cr),through static leaching tests,SEM,and XRD analysis.The results indicate that:① Cr exhibits the highest stability,followed by Pb and Zn,while Cu is the most susceptible to morphological transformation due to environmental and chemical influences.② The long-term stability of the backfill is highly dependent on the ambient pH.Specimens with a binder-to-tailings ratio of 1∶10 achieved the highest 90 d strength(2.11 MPa)under neutral conditions(pH=7),whereas those with a 1∶20 ratio showed the lowest strength(0.63 MPa)in an alkaline environment(pH=10).Acidic conditions induced early-stage erosion,while alkalinity led to late-stage expansion and degradation.③ The binder-to-tailings ratio significantly influences the immobilization efficiency.The highest leaching concentrations for Pb,Cu,Zn,and Cr were observed at the 1∶20 ratio,measuring 0.000 95,0.94,0.86,and 0.014 7 mg/L,respectively—approximately 2 to 3 times higher than those at the 1∶10 ratio.Despite this increase,all values complied with the Class III standards of the"Quality Standard for Groundwater"(GB/T 14848-2017).This research clarifies the interrelationships among environmental conditions,mix proportion,and backfill performance,providing a critical basis for the design of backfill in green mining.

焦华喆;李振龙;张庆澳;靳翔飞;许军强;王哲;王建栋;李公成;龚剑;周淼

河南理工大学 土木工程学院,河南 焦作 454003||焦作千业新材料有限公司,河南 焦作 454003河南省第一地质矿产调查院有限公司,河南 洛阳 471023河南理工大学 土木工程学院,河南 焦作 454003河南理工大学 土木工程学院,河南 焦作 454003河南省第一地质矿产调查院有限公司,河南 洛阳 471023河南省第一地质矿产调查院有限公司,河南 洛阳 471023北京科技大学 资源与安全工程学院,北京 100083山东理工大学 资源与环境工程学院,山东 淄博 255049郑州工程技术学院 土木工程学院,河南 郑州 450044河南理工大学 土木工程学院,河南 焦作 454003

矿业与冶金

强度特性重金属固化胶材掺量微观结构演变水化产物

strength characteristicsheavy metal immobilizationbinder dosagemicrostructural evolutionhydration product