基于防水黏结性能的再生砖粉砂浆外加剂调控化及纤维增强性能研究OA

Study on Admixture Regulation and Fiber-Reinforced Properties of Recycled Brick Powder Mortar Based on Waterproof and Bonding Performances

中文摘要英文摘要

针对仿古建筑饰面墙体在水分与可溶盐迁移作用下易引发材料酥解、黏结力下降等问题,采用"砌体-防水黏结砂浆-青砖面砖"的复合墙体构造作为一种有效的解决方案,利用再生砖粉作为部分胶凝材料,并复掺聚合物等组分,制备防水黏结砂浆.以正交试验结合层次分析法优化憎水剂、消泡剂和减水剂配比,并研究聚丙烯纤维长度及掺量对砂浆性能和微观结构的影响.结果表明,在再生砖粉-硅灰-水泥复合胶凝体系中,最优外加剂组合为憎水剂0.2%、消泡剂0.6%、减水剂1.0%,该组合可有效提高砂浆拉伸粘结强度,吸水率为4.5%,同时颗粒分散状态和孔隙结构得到改善.在最优外加剂组合基础上,PP纤维主要通过桥接微裂缝和降低孔隙连通性改善砂浆性能,其中9 mm纤维在0.2%~0.3%掺量下综合效果较优,当掺量为0.3%时,涂层抗渗压力达到2.6 MPa,较未掺纤维对照组提高约24%.

To address issues such as material crumbling and reduced bond strength in the facade walls of historic-style buildings caused by the migration of moisture and soluble salts,this paper proposes a composite wall structure consisting of"masonry-waterproof bonding mortar-blue brick facing"as an effective solution.The waterproof bonding mortar is prepared using recycled brick powder as a partial cementitious material,blended with polymers and other components.An orthogonal experiment combined with the Analytic Hierarchy Process(AHP)was used to optimize the proportions of water-repellent agent,defoamer,and water-reducing agent,and the effects of polypropylene fiber length and dosage on the mortar's properties and microstructure were investigated.The results indicate that,in the recycled brick powder-silica fume-cement composite binder system,the optimal admixture combination is 0.2%water-repellent agent,0.6%defoamer,and 1.0%water-reducing agent.This combination effectively improves the mortar's tensile bond strength,reduces the water absorption rate to 4.5%,and simultaneously enhances particle dispersion and pore structure.Based on this optimal admixture combination,PP fibers primarily improve mortar performance by bridging microcracks and reducing pore connectivity.Among these,9-mm fibers exhibited superior overall performance at incorporation levels of 0.2%to 0.3%.When the incorporation level was 0.3%,the coating's impermeability pressure reached 2.6 MPa,representing an increase of approximately 24%compared to the control group without fiber addition.

周理安;赵晨妍;杨灿;陈晶晶

北京建筑大学 土木与交通工程学院,北京 100044||住房和城乡建设部建筑垃圾资源化工程技术创新中心,北京 100044北京建筑大学 土木与交通工程学院,北京 100044北京建筑大学 土木与交通工程学院,北京 100044北京建筑大学 土木与交通工程学院,北京 100044

建筑与水利

再生砖粉防水黏结砂浆层次分析法聚丙烯纤维

recycled brick powderwaterproof bonding mortaranalytic hierarchy processpolypropylene fiber