Synergistic inhibition effect of fluoride and caffeiate on LAZ931 Mg alloy corrosionOA

中文摘要

Improving the corrosion resistance of magnesium-lithium(Mg-Li)alloys is pivotal for expanding their prospective utilization in lightweight structural materials.This research focused on evaluating the corrosion inhibition effectiveness of a composite corrosion inhibitor comprising sodium fluoride(NaF)and caffeic acid(CA)on the LAZ931 alloy in a 3.5 wt.%NaCl solution.The results demonstrated that NaF alone is insufficient to prevent localized corrosion of the alloy.Remarkably,the addition of 0.001 M caffeic acid to a 0.05 M NaF solution significantly increased the corrosion inhibition efficiency from 54.36%to 88%.This substantial improvement in corrosion resistance can be credited to the formation of the dense protective NaMgF_(3) deposition products on the sample surface.This study offers a novel approach to the design of corrosion inhibitors for duplex Mg alloys,emphasizing the synergistic effect between NaF and CA in augmenting corrosion protection.

Yishun Tian;Tiancai Kong;Shuya Mao;Di Mei;Zhipeng Liu;Jinxue Liu;Yang Xiao;Liguo Wang;Shijie Zhu;Shaokang Guan

School of Materials Science and Engineering&Henan Province Key Laboratory of Advanced Light Alloys,Zhengzhou University,Zhengzhou 450001,ChinaSchool of Materials Science and Engineering&Henan Province Key Laboratory of Advanced Light Alloys,Zhengzhou University,Zhengzhou 450001,ChinaSchool of Materials Science and Engineering&Henan Province Key Laboratory of Advanced Light Alloys,Zhengzhou University,Zhengzhou 450001,ChinaSchool of Materials Science and Engineering&Henan Province Key Laboratory of Advanced Light Alloys,Zhengzhou University,Zhengzhou 450001,ChinaSchool of Materials Science and Engineering&Henan Province Key Laboratory of Advanced Light Alloys,Zhengzhou University,Zhengzhou 450001,China Zhengzhou Light Alloy Institute Co.,Ltd.,Zhengzhou 450041,ChinaZhengzhou Light Alloy Institute Co.,Ltd.,Zhengzhou 450041,ChinaSchool of Materials Science and Engineering&Henan Province Key Laboratory of Advanced Light Alloys,Zhengzhou University,Zhengzhou 450001,China Zhongyuan Critical Metals Laboratory(Zhengzhou University),Zhengzhou 450001,China Zhengzhou Light Alloy Institute Co.,Ltd.,Zhengzhou 450041,ChinaSchool of Materials Science and Engineering&Henan Province Key Laboratory of Advanced Light Alloys,Zhengzhou University,Zhengzhou 450001,China Zhongyuan Critical Metals Laboratory(Zhengzhou University),Zhengzhou 450001,ChinaSchool of Materials Science and Engineering&Henan Province Key Laboratory of Advanced Light Alloys,Zhengzhou University,Zhengzhou 450001,China Key Laboratory of Materials Processing and Mold(Ministry of Education),Zhengzhou 450002,ChinaSchool of Materials Science and Engineering&Henan Province Key Laboratory of Advanced Light Alloys,Zhengzhou University,Zhengzhou 450001,China Key Laboratory of Materials Processing and Mold(Ministry of Education),Zhengzhou 450002,China

矿业与冶金

Magnesium-lithiumCorrosion inhibitor mixtureLocalized corrosionMechanical properties

《Journal of Magnesium and Alloys》 2026 (4)

P.408-421,14

the Joint Fund Project of Henan Provincial Science and Technology Research and Development Plan(242301420036)the National Natural Science Foundation of China(52301107)the Domain Foundation of Equipment Advance Research of the 14th Five-year Plan(50922010302)“Insight Action”project(619672D6)supported by the Project of Zhongyuan Critical Metals Laboratory.

10.1016/j.jma.2025.03.015