机制砂絮凝剂残留的混凝土外加剂适配处理技术研究OA
Study on the Treatment Technology of Residual Concrete Additive of Mechanical Sand Flocculant
为解决湿法制砂工艺中絮凝剂残留,导致机制砂混凝土工作性能、力学性能及耐久性下降的问题,文中以泉州阳江水质净化提升工程为例,以含不同残留量聚丙烯酞胺(PAM)、聚合氯化铝(PAC)的机制砂为细骨料,选用某企业生产的长支链超保坍母液型聚羧酸减水剂,对混凝土外加剂适配性进行研究.结果表明,当 PAM 残留量为0.5‰时,将减水剂掺量从1.0%提升至1.25%,复配1.0‰十六烷基三甲基氯化铵及1.5‰聚乙二醇,并将砂率从38%提高至41%,混凝土初始坍落度可从170 mm 恢复至200 mm,1 h 坍落度损失降至30 mm,28 d 抗压强度达38.5 MPa,抗渗等级达到P8,抗冻等级达F200,满足工程要求.该研究为含絮凝剂残留机制砂的混凝土应用提供了外加剂适配技术方案.
To address the degradation of workability,mechanical properties,and durability in manufactured sand concrete caused by flocculant residues in wet sand production processes,this study conducted compatibility research using manufactured sand with varying residual polyacrylamide(PAM)and polyaluminum chloride(PAC)content as fine aggregates,along with a long-chain super-sagging mother liquor-type polycarboxylate superplasticizer produced by a manufacturer,as exemplified by the Quanzhou Yangjiang Water Purification Enhancement Project.Results demonstrated that when the PAM residue in manufactured sand was 0.5‰,increasing the dosage of the long-chain super-sagging mother liquor-type polycarboxylate superplasticizer from 1.0%to 1.25%,combined with 1.0‰ cetyltrimethylammonium chloride and 1.5‰ polyethylene glycol,while raising the sand ratio from 38%to 41%,the initial slump of concrete could recover from 170 mm to 200 mm,with 1-hour slump loss reduced to 30 mm.The 28-day compressive strength reached 38.5 MPa,achieving P8 water resistance and F200 frost resistance,meeting engineering requirements.This study provides an additive compatibility technical solution for concrete applications involving manufactured sand with flocculant residues.
林金荣
福建省建筑科学研究院有限责任公司,福建 福州 350108||福建省绿色低碳建筑技术重点实验室,福建 福州 350108
建筑与水利
机制砂絮凝剂残留混凝土外加剂长支链超保坍母液
Mechanism sandFlocculant residueConcrete admixtureLong-chain super-sagging mother liquor
《江西建材》 2026 (4)
68-72,5
评论