GFRP筋力学性能试验研究OA
Experimental Study on Mechanical Properties of Glass Fiber-reinforced Polymer Bar
为改善玻璃纤维增强聚合物(GFRP)筋在拉伸试验中因端部应力集中导致的夹持碎裂问题,文中采用钢套筒灌浆锚固技术对3 根GFRP 筋试件进行了处理,并以1 根普通GFRP 筋试件作为对照,开展单向拉伸对比试验.结果表明,钢套筒灌浆锚固能够有效分散夹持应力,使试件由夹持端碎裂破坏转变为筋材中部拉断破坏,极限抗拉强度在755~760 MPa,真实地反映了GFRP 筋的材料性能;GFRP 筋荷载-位移曲线在破坏前呈线性增长,无明显塑性变形阶段,表现出典型脆性特征,弹性模量稳定在45.7~46.2 GPa.本研究验证了钢套筒灌浆锚固技术在 GFRP 筋拉伸试验中的有效性,为其在工程中的锚固设计与性能评估提供了试验依据.
To mitigate the gripping failure and crushing of Glass Fiber-Reinforced Polymer(GFRP)bars at the ends during tensile tests,caused by stress concentration,this study employed a steel sleeve grouting anchorage technique.Three GFRP bar specimens were treated with this method and subjected to monotonic tensile tests,with one untreated GFRP bar serving as a control.The results demonstrated that the steel sleeve grouting anchorage effectively distributed the gripping stresses,shifting the failure mode from crushing at the grips to tensile fracture in the mid-length of the bar.The ultimate tensile strength of the anchored specimens ranged from 755 to 760 MPa,which more accurately reflects the true material properties of the GFRP bars.The load-displacement curves of the GFRP bars exhibited linear behavior up to failure without a distinct plastic deformation stage,indicating typical brittle characteristics.The elastic modulus remained stable within a range of 45.7 to 46.2 GPa.This research validates the effectiveness of the steel sleeve grouting anchorage technique for tensile testing of GFRP bars,providing an experimental basis for their anchorage design and performance evaluation in engineering applications.
李志强;丁志伟;刘佳琪;黄和富
江西建工第二建筑有限责任公司,江西 南昌 330001江西建工第二建筑有限责任公司,江西 南昌 330001江西建工第二建筑有限责任公司,江西 南昌 330001南昌大学工程建设学院,江西 南昌 330031
建筑与水利
GFRP筋钢套筒灌浆锚固性能单向拉伸荷载-位移曲线
GFRP barsSteel sleeve groutingAnchorage performanceUniaxial tensionLoad-displacement curve
《江西建材》 2026 (4)
35-38,4
评论