硅粉/硅烷偶联剂复合改性市政给排水管道接口连接砂浆耐腐蚀性能研究OA
Study on Corrosion Resistance Performance of Municipal Water Supply and Drainage Pipe Interface Connection Mortar Modified by Silicon Powder/Silane Coupling Agent Composite
为提升市政排水管道系统长期运行稳定性,文中设计不同配合比硅烷偶联剂掺量砂浆,系统分析了硅烷偶联剂掺量对管道接口砂浆抗压、抗折性能、抗渗性能及耐腐蚀性能的影响规律.结果表明,随着硅烷掺量的增加,砂浆抗压、抗折强度均呈现先增大后减小的变化趋势;吸水率和抗渗压力分别呈先降后增和先增后降的变化趋势.在 Na2 SO4 溶液中,1.5%硅烷掺量砂浆质量损失率最低,抗压、抗折耐腐蚀系数最高.综上,确定采用硅粉掺量为8%、硅烷偶联剂掺量为1.5%复合改性方案为最优配合比.
To enhance the long-term operational stability of municipal drainage pipeline systems,by designing mortars with different mix ratios and silane coupling agent dosages,the influence laws of silane coupling agent dosages on the compressive strength,flexural strength,impermeability and corrosion resistance of pipe interface mortars were systematically analyzed.The results show that with the increase of silane dosage,both the compressive and flexural strengths of the mortar present a trend of first increasing and then decreasing.The water absorption rate and impermeability pressure respectively showed a trend of first decreasing and then increasing,and first increasing and then decreasing.In the Na2SO4 solution,the mortar with a 1.5%silane content has the lowest mass loss rate and the highest compressive,flexural and corrosion resistance coefficients.In conclusion,it is determined that the optimal mix ratio is the composite modification scheme with a silicon powder dosage of 8%and a silane coupling agent dosage of 1.5%.
杨知
宿迁市城市规划设计研究院有限公司,江苏 宿迁 223800
建筑与水利
排水管接口连接砂浆硅粉硅烷偶联剂耐腐蚀性能配合比优化
Drainage pipeInterface connection mortarSilicon powder silane coupling agentCorrosion resistanceMix ratio optimization
《江西建材》 2026 (2)
65-67,73,4
评论