细骨料掺量对SHCC基体粉体颗粒级配的影响规律研究OA
Research on the Influence of Fine Aggregate Dosage on Concrete Performance under Different Sand-cement Ratios
为研究细骨料对SHCC基体性能的影响,文中通过制备不同细骨料掺量的混凝土试件并分别进行扩展度、流动度和力学试验,系统研究了不同砂胶比下细骨料掺量对基体粉体颗粒级配、工作性能及力学性能的影响.试验结果表明,随着砂胶比增大,粉体颗粒整体粗化,各粒径累积通过率均呈下降趋势;细骨料掺量的增加对最佳水胶比有明显影响,砂胶比从 0.36 增至 0.84 时,最佳水胶比由0.320 递增至0.420;SHCC的抗压强度、抗折强度和拉伸应变随砂胶比增加先增后降,砂胶比为0.6 时,力学性能最优,抗压强度、抗折强度和拉伸应变分别提升至36.59 MPa、25.79 MPa和5.51%;最终确定SHCC最优配合比为水泥∶粉煤灰∶细骨料∶水∶减水剂=1∶2∶1.8∶1.065∶0.045 vol%.
To study the influence of fine aggregates on the properties of SHCC matrix,by preparing concrete specimens with different fine aggregate dosages and conducting expansion,fluidity and mechanical testsrespectively,the effects of fine aggregate dosages under different sand-binder ratios on the particle size distribution,working performance and mechanical properties of the matrix powder were systematically investigated.The test results show that:With the increase of the sand-binder ratio,the powder particles become coarser as a whole,and the cumulative pass rates of each particle size all show a downward trend.The increase in the dosage of fine aggregates has a significant impact on the optimal water-binder ratio.When the sand-binder ratio increases from 0.36 to 0.84,the optimal water-binder ratio increases from 0.320 to 0.420.The compressive strength,flexural strength and tensile strain of SHCC increase first and then decrease with the increase of the sand-binder ratio.When the sand-binder ratio is 0.6,the mechanical properties are the best.At this time,the compressive strength,flexural strength and tensile strain increase to 36.59 MPa,25.79 MPa and 5.51%respectively.The final determined optimal mix ratio of SHCC is cement:fly ash:fine aggregate:water:water reducing agent=1:2:1.8:1.065:0.045 vol%.
魏子阳
华北水利水电大学,河南 郑州 450000
建筑与水利
SHCC配合比设计颗粒级配工作性能力学性能
SHCCMix proportion designParticle gradationWorking performanceMechanical properties
《江西建材》 2026 (1)
86-89,4