中文摘要英文摘要

随着中国工业汉麻年产量及其全球市场份额增长,工业汉麻的多用途开发成为未来发展的重要趋势.通过化学成分测定可得工业汉麻的纤维素含量高达 59.36%,这为纳米纤维素的制备提供了可能.为拓宽工业汉麻的应用领域,本文采用多步化学提纯处理,分别结合 2,2,6,6-四甲基哌啶-1-氧基自由基(2,2,6,6-tetramethylpiperidine-1-oxyl radical,TEMPO)氧化和硫酸水解制备了氧化纳米纤维素(TCNF)、酸水解纳米纤维素(SCNC)和含木质素的水解纤维素(LCNC).采用傅里叶红外光谱、X射线衍射和热重分析对其进行了表征.探究了次氯酸钠用量、预处理过程中氢氧化钠质量分数和酸水解反应时间对所制备纳米纤维素Zeta电位和粒径的影响.试验结果表明,SCNC的Zeta电位绝对值可达 29.59 mV,同时其粒径较小,且其悬浮液在相同的分散条件下,静置24.0 h仍能保持良好的分散稳定性;其结晶度最高可由原麻的24.6%提高到68.1%.所制备的3 种纳米纤维素的基本官能团组成和晶体形态与原麻相比无变化.由于酯基和羧基的引入,纳米纤维素的初始分解温度和最大分解速率温度相较于原麻有所降低,但仍可满足实际应用所需的热稳定性.

As the annual production of industrial hemp in China increases and its global market share grows,its multipurpose development has become an important trend for future development.The cellulose mass fraction of industrial hemp was found to be as high as 59.36%by chemical composition determination,providing a possibility for the production of nanocellulose.To broaden the application field of industrial hemp,the 2,2,6,6-tetramethylpiperidine-1-oxyl radical(TEMPO)-oxidized nanocellulose(TCNF),sulfuric acid hydrolyzed nanocellulose(SCNC),and lignin-containing hydrolyzed nanocellulose(LCNC)were prepared by multi-step chemical purification pretreatment combined with TEMPO oxidation and sulfuric acid hydrolysis,respectively.They were characterized by Fourier transform infrared(FTIR)spectroscopy,X-ray diffraction(XRD),and thermogravimetric analysis(TGA).The effects of the sodium hypochlorite volume,sodium hydroxide mass fraction in the pretreatment process,and acid hydrolysis reaction time on the Zeta potential and particle size of the prepared nanocellulose were investigated.The absolute value of the Zeta potential of SCNC could reach 29.59 mV,and the particle size was small.The suspension could still maintain good dispersion stability after standing for 24.0 h under the same dispersion conditions.The basic functional group composition and crystal morphology of TCNF,SCNC,and LCNC did not change compared with the raw hemp,and the highest crystallinity increased from 24.6%to 68.1%.Due to the introduction of ester and carboxyl groups,the initial degradation temperature and the temperature at the maximum mass loss rate of the nanocellulose were lower than those of the raw hemp,but the nanocellulose still maintained the thermal stability for practical applications.

王燕鸽;古宇;赵树元;秦智慧;刘柳;张瑞云

东华大学 纺织学院,上海 201620||东华大学 纺织面料技术教育部重点实验室,上海 201620东华大学 纺织学院,上海 201620||东华大学 纺织面料技术教育部重点实验室,上海 201620东华大学 纺织学院,上海 201620||东华大学 纺织面料技术教育部重点实验室,上海 201620东华大学 纺织学院,上海 201620||东华大学 纺织面料技术教育部重点实验室,上海 201620东华大学 纺织面料技术教育部重点实验室,上海 201620||东华大学 纺织科技创新中心,上海 201620东华大学 纺织学院,上海 201620||东华大学 纺织面料技术教育部重点实验室,上海 201620||东华大学 纺织科技创新中心,上海 201620

轻工纺织

工业汉麻纳米纤维素酸水解TEMPO氧化

industrial hempnanocelluloseacid hydrolysisTEMPO oxidation

《东华大学学报(英文版)》 2026 (1)